Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C @Thickness 6.35 mm |
320 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne LubriOne™ AT-000/10T Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ISO 75 |
Nilit FRIANYL B63 HH Nylon 6 for injection molding Nylon 6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM D648 |
Qualchem Danaprop PP1GF-30 Polypropylene, 30% Glass Fiber Polypropylene (co-polymer) reinforced with glass fiberInformation provided by Qualchem Zrt. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | Unannealed, 0.125 in bars; ASTM D648 |
PolyOne Edgetek® GF 5209 10 FPS 15 BLACK 30 A 1 Acetal-Copolymer, Glass Filled
(discontinued **) PRELIMINARY DATA SHEETDescription/Features:Glass Fiber ReinforcedBlackInformation provided by PolyOne Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM D648 |
Kolon Kocetal® TC704 Reinforced Grade Acetal Copolymer
(Unverified Data**) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM D648 |
LATI LATILUB 73/13-01M Polyoxymethylene Base (POM), 1% Molybdenum Disulfide Self Lubricating Plastic
(Unv Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C @Thickness 6.40 mm |
320 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® ML5472 PC Gamma sterilization resistant. High heat (PPC). Available in natural color only. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM D648 |
LG Chemical LUCEL FW-710F Friction and Wear Resistant POM, PTEE filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C @Thickness 6.40 mm |
320 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical LUCEL N109WR POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Automotive Air-conditioner Valve, Fuel Tank Cap, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C @Thickness 6.40 mm |
320 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical LUCEL N127LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | DIN 53461; ASTM D648 |
Kolon KOPA® KN173HI4 High Impact Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ISO 75-1/-2 |
Lanxess Pocan® B 1300 000000 PBT PBT, non-reinforced, injection molding, extrusion |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C @Thickness 3.17 mm |
320 °F @Thickness 0.125 in |
un-annealed; ASTM D648 |
MRC Polymers MAXTELâ„¢ 600 GF30 TPO, 30% Glass Fiber Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | |
LATI Latan 13 POM Polyoxymethylene (POM). Unfilled. Medium viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP GF15 CC 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C @Thickness 3.20 mm |
320 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GTX GTX6009 PPE+PS+PA6 (Asia Pacific) PA6 based unfilled GTX for Wheel cover |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C @Thickness 3.17 mm |
320 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
Chase Plastics CP Pryme® AC100-9 Acetal Copolymer Molding Resin Information provided by Chase Plastics. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | DIN 53461 |
Polyram PlusTek PB891 Nylon 6, Impact Modified Impact modified polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | DIN 53461 |
Polyram RamSter PF702 PBT, UV Stabilized UV stabilized, medium viscosity PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | DIN 53461 |
Polyram RamTal PM7109 Acetal, UV Stabilized UV stabilized polyacetal copolymer for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | Flatw 80x10x4, sp=64 mm; ISO 75/Bf |
Eurostar Staramide R1000EI2 PA66, Impact Modified, Injection Molded Staramide R1000EI2 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI010)Information provided by Eurostar. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | Annealed; ASTM D648 |
Engineered Plastics EPPC 314C Polycarbonate Clear; extrusion/blow molding grade. Property values below represent typical values. Information provided by Engineered Plastics Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | |
Arkema Group Orgalloy® R 6600 Nylon 66 Alloy, Rigid Grade (Conditioned) Rigid polyamide 6.6 alloy: easy to process, low moisture absorption, chemical resistance (no known solvents).ISO data provided by the manufacturer, Arkema. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM D648 |
Asahi Kasei Thermylene® P6-30FG-0155 30% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM D648 |
Asahi Kasei Thermylene® P6-40FM-B269 40% Glass/Mineral Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | ASTM D648 |
Ashley Polymers Ashlene® 851 Nylon 6, High Viscosity High viscosity for blown film, tubing, rods and shapes and blow molding. Has highest puncture resistance and clarity. FDA and NSF approved.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® FG7301 NC010 Nylon 6
(Unverified Data**) Zytel® FG7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications. It has been developed for consideration into applications such as parts for the food industry.In.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | |
LATI Latigray 82-05 CX/90 PA 12 Radiopaque compound based on Polyamide 12 (PA12). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 °C | 320 °F | |
LATI Latimass 82-03 D110 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |