Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | ASTM D648 |
Proto3000 Duraform® PA Selective Laser Sintering (SLS®) Prototyping Polymer Description: Durable polyamide (nylon) material for real-world physical testing and functional useFeatures: Excellent surface resolution and feature detailEasy-to-processCompliant with USP Class VI .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | Annealed; ISO 75-1/-2 |
DuPont Performance Polymers Crastin® FG6129 NC010 PBT
(Unverified Data**) Crastin® FG6129 NC010 is an unreinforced, high viscosity polybutylene terephthalate resin for extrusion and injection molding. It has been developed for consideration into applications such as part.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | Annealed; ISO 75-1/-2 |
DuPont Performance Polymers Crastin® S600F40 NC010 PBT
(Unverified Data**) Crastin® S600F40 NC010 is an unreinforced, lubricated, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 - 192 °C | 356 - 378 °F | Average value: 185 °C Grade Count:3 |
Overview of materials for Nylon 11 with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are includ.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | DIN 53461; ASTM D648 |
Kolon KOPA® KN126 General Purpose Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | DIN 53461; ASTM D648 |
Kolon KOPA® KN170SA General Purpose Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | DIN 53461; ASTM D648 |
Kolon KOPA® KN177N Nylon Extrusion Resin Excellent transparent & flexible copolyamide, typical applications are fishing nets & fishing linesInformation provided by US distributor, API-Kolon. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C @Thickness 3.20 mm |
356 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON IS000XXL PA6.12 LNP* STAT-KON* IS000XXL is a compound based on Nylon 6/12 containing Stainless Steel Fibers. Added features of this material include: Food Contact Compliant Raw Materials, Metal Detectable, Electr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP GF004 PSU LNP* Thermocomp* GF004 is a compound based on Polysulfone resin containing 20% Glass Fiber. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C @Thickness 3.20 mm |
356 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics NORYL HH180 PPE+PS Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C @Thickness 3.20 mm |
356 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON 9X04323 PPE+PA66 (Asia Pacific) LNP* Stat-kon* 9X04323 is a compound based on Noryl GTX resin,Added features of this material include: Electrically Conductive. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | ISO 75-1/2 |
Suzhou Hipro Polymers Hiprolon® 400 MC HLS G30 Nylon, 30% glass fiber filled Hiprolon® 400 MC HLS G30 is a specialty long chain polyamide compound reinforced with 30% chopped glass fiber for injection molding. It contains some bio-renewable resources Features: high dime.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | ISO 179 |
CP-Polymer-Technik Wellamid® 6000 SCP Nylon 6, Finely Crystalline, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | annealed; ISO 75-1/-2 |
DuPont Performance Polymers Crastin® FG6130 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced High Viscosity Polybutylene Terephthalate Developed for Food Contact Applications and Extrusion and Injection Molding Crastin FG6130 NC010 is an unreinforced medium high viscosity polyb.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | annealed; ISO 75-1/-2 |
DuPont Performance Polymers Crastin® FG6134 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced Medium Viscosity Polybutylene Terephthalate Developed for Food Contact Applications Crastin® FG6134 NC010 is an unreinforced medium viscosity polybutylene terephthalate resin for injec.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | Flatw 80x10x4, sp=64 mm; ISO 75/Bf |
Eurostar Staramide PB00A PA6, 50% Glass Bead Filled, Injection Molded Staramide PB00A is a 50% Glass Bead Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | ISO 75 |
BASF Ultramid® B3ZG3 BK30564 15% Glass Filled PA6 (Dry) Ultramid B3ZG3 BK30564 is an impact-modified, pigmented black, 15% glass fiber reinforced injection molding PA6 grade. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | HDT/B; ISO 75-2 |
Akro-Plastic Akromid® B3 (2500) PA 6 Dry AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | ISO 75-1/-2 |
BASF Ultramid® B3K BK00464 PA6 (Dry) Description: Easy flowing and stabilized injection-molding grade used for technical parts with wall thicknesses >2 mm, e.g. machinery components, fans and power tool housings.Information provided by.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | ASTM D648 |
Beijing Ranger Chem PBT-201-G0 272 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | ASTM D648 |
Beijing Ranger Chem PBT-201-G0 291 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | ISO 75-1/-2 |
DSM Akulon® F232-DH Nylon 6 (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | ISO 75-1/2 |
Eurotec® Tecomid® NB40 MR25 NL IL PA 6 25% mineral reinforced, impact modified Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | ISO 75 |
Eurotec® Tecomid® NB40 NL E PA6, unfilled, natural Information provided by Eurotec® |
|||
Deflection Temperature at 0.46 MPa (66 psi) | >= 180 °C | >= 356 °F | DIN 53461 |
Polyram PlusTek RA502 Nylon 6.6, Flame Retardant Polyamide 6.6, flame retardant for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP GF004 PSU (Asia Pacific) LNP* Thermocomp* GF004 is a compound based on Polysulfone resin containing Glass Fiber. |