Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | |
Nylene® PA6/6 Homopolymer 134 HSL Nylon 6/6 Low Viscosity Nucleated Grade; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ISO 75, ASTM D648 |
Nilit Nilamid A3 N H2 Nucleated, Heat Stabilized Nylon 66 Description: Nilamid A3 N H2 is a nucleated, heat stabilized NYLON 66 with excellent flow characteristics and very fast cycle time. It is widely used throughout many industries for mass production a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ISO 75 |
Nilit FRIANYL C73 GV40 Nylon 6.6/6 for injection molding, 40% glass fiber reinforced Nylon 6.6/6 for injection molding, medium viscosity.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Ensinger ENSILON® 6/6 Extruded Nylon 6/6 (PA66)
(discontinued **) ENSILON materials have high mechanical strength and superior resistance to wear and organic chemicals.Ensilon grades have been replaced by Tecamid.Information supplied by Ensinger, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylon® N1000NL Nylon 6/6 (Cond)
(discontinued **) Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | DIN 53461; ASTM D648 |
Kolon KOPA® KN333G15HI Multi Reinforced Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | DIN 53461; ASTM D648 |
Kolon KOPA® KN333HS Heat Resistant Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C @Thickness 6.40 mm |
455 °F @Thickness 0.252 in |
ASTM D648 |
Kingfa PA66-T15 15% Mineral Filled PA66 Features:Good size stabilityLow tendency to wrapGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower toolsSport applianceInformation Provided by Kingfa Sci. & .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | |
LATI Latamid 66 H2 G/25-V0CT4 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Lat.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP RX05487 PA 66 LNP* LUBRICOMP* RX05487 is a compound based on Nylon 66 containing 10% Aramid Fiber, 10% Lubricant. Added features of this material are: Low Warpage, Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP UAL23AS PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UAL23AS is a compound based on Polyphthalamide resin containing Aramide Fiber, PTFE. Added features include : Internally Lubricated, Heat Stabilized. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOTUF VF004S PA 66 LNP THERMOTUF* VF004S is a compound based on Nylon resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C @Thickness 3.20 mm |
455 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C @Thickness 3.20 mm |
455 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Asia Pacific) Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ISO 75 |
Polyram PlusTek PA355M6 Nylon 6.6 for Injection Molding, 30% Mineral Filled, Flame Retardant 30% Minerals filled, flame retardant Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | 0.455 MPa |
Toyobo ECOVYLOPET® EMC2310 PET Bottle Recycling Grade, 10% Glass Reinforced Features: PET Bottle Recycling Grade, 10% Glass Fiber Reinforced, General PurposeApplications: Automobile engine head coversHot platesVending machine partsUmbrella ribsInformation provided by Toyobo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | 0.455 MPa |
Toyobo ECOVYLOPET® EMC2311 PET Bottle Recycling Grade, 10% Glass Reinforced Features: PET Bottle Recycling Grade, 10% Glass Fiber Reinforced, General PurposeApplications: Automobile engine head coversHot platesVending machine partsUmbrella ribsInformation provided by Toyobo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Unitika UNILATE® 1 PC PET Standard gradeUNILATE® products are plate materials prepared by using a polyethylene terephthalate (PET resin) as the main component, blending it with glass staple fiber, inorganic filler, and othe.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Ensinger Tecamid® 6/6 Nylon (PA66) Type 6/6 is a general purpose standard grade nylon. Extruded in natural and black. (Weather Resistant Black Grade is also available.)Information provided by Ensinger, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® FR7025V0F NC010 Nylon 66
(Unverified Data**) Zytel® FR7025V0F NC010 is a flame retardant polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuPont Performance.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Clariant Renol PA112 Nylon 66, Nucleated Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Clariant Renol PA113 Nylon 66, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
E-Polymers TEKAMID® TA250FR , Flame Retardant Un-Reinforced PA66, DAM Flame retardantInformation provided by E-Polymers Co. Ltd. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Be |
Eurostar Starflam AFR662B1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding Starflam AFR662B1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
E-Polymers TEKAMID® TA210F Fast Crystallinity PA66, DAM Fast crystallinityInformation provided by E-Polymers Co. Ltd. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM Test |
BASF Petra® 130 BK-112 30% Glass Filled PET Petra 130 BK-112 is a 30% glass fiber reinforced, black pigmented polyethylene terephthalate injection molding compound. It exhibits a combination of performance properties including good strength .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Ashley Polymers Ashlene® 528L Nylon 66 General purpose injection molding grade.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Ashley Polymers Ashlene® 528LW Nylon 66 General purpose injection molding grade.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Cheng Yu Plastic E2315 Flame Retardant PET, 15% Glass Fiber |