Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Europe-Africa-Middle East) CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of propertiesThis data was supplied by.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Asia Pacific) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPC T1035 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C @Thickness 3.20 mm |
243 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Cycoloy® XCY480 PC+ABS (Europe-Africa-Middle East) High flowThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C @Thickness 3.18 mm |
243 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Edgetek® X TR2-20GF/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | |
Ineos ABS TRIAX® 1408 GF ABS/Nylon Blend, Injection Grade, As Conditioned
(discontinued **) Standard injection molding grade, easy flow, easy mold release, fast setting.Applications: Thin walled engineering parts. Automotive sector: air filters, switch and connector parts for car electric... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycoloy® C1000HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C1000HF is a general purpose PC+ABS blend specially developed for thin wall applications requiring a high flow with a good balance of properties. It is suitable for applications in the autom.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.This .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | ASTM D648 |
Flint Hills P4G4K-205 Homopolymer Polypropylene Features: Clarified material. Product does not contain animal derived components. Phthalate-free.Applications: Cast FilmInformation provided by Flint Hills Resources. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C @Thickness 6.40 mm |
243 °F @Thickness 0.252 in |
ASTM D648 |
LG Chemical LUCON CP6052 PC/ABS+CNT Description Injection Molding Grade, PC/ABS+CNT, Electrostatic Dissipation, Low Surface Resistivity, Improved Impact StrengthApplication: Laser diode Tray, ATM parts, Telecommunication Station Housi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C @Thickness 6.40 mm |
243 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical Lupox® TE5000GU PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Door Garnish, Door Handle)CAS No. 137050-02-03, 24968-12-5 and 103598-77-2Info.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | ISO 75/Bf |
Solvay TECHNYL® C 507XT PA6, DRY Description: Unreinforced polyamide 6, heat stabilized, very high viscosity, for extrusion.Available in: Europe Product Applications: It is suitable for extruded semi-finished products, such as: Rod.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C @Thickness 3.20 mm |
243 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL HS2000X PPE+PS PPE+PS blend. 17% Mineral reinforced. Non-brominated, non-chlorinated FR system. UL94 V0 and 5VA listing. UL746C f1. Radiant panel listing. Dielectric strength. Dimensional stability. Suitable for E.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C @Thickness 3.20 mm |
243 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Noryl PKN4766 PPE+PS (Asia Pacific) PPE+PS. Translucent. FDA compliant. High flow. Extrusion. Microwavable. Food packaging uses.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Thermocomp ZF0041XC PPE+PS (Europe-Africa-Middle East) LNP* THERMOCOMP* ZF0041XC is a compound based on PPE+PS Blend resin containing Glass Fiber and Flame retardant. Added features include Flame Retardant.This data was supplied by SABIC-IP for the Euro.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 2661 Injection Molding Grade Mineral Fortified Polypropylene DescriptionPolyfort® FPP 2661 is a injection molding grade mineral fortified impact enhanced polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 2661 Injection Molding Grade Mineral Fortified Polypropylene DescriptionPolyfort® FPP 2661 is a injection molding grade mineral fortified impact enhanced polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 2661 Injection Molding Grade Mineral Fortified Polypropylene DescriptionPolyfort® FPP 2661 is a injection molding grade mineral fortified impact enhanced polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 2661 Injection Molding Grade Mineral Fortified Polypropylene DescriptionPolyfort® FPP 2661 is a injection molding grade mineral fortified impact enhanced polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 2661 Injection Molding Grade Mineral Fortified Polypropylene DescriptionPolyfort® FPP 2661 is a injection molding grade mineral fortified impact enhanced polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® BM7300THS BK317 Nylon 6
(Unverified Data**) Zytel® BM7300THS is an unreinforced, heat stabilized, lubricated, toughened polyamide 6 for blow molding.Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | ASTM D648 |
Aclo Accutech Polypropylene Homopolymer HP0336M10CL Mica Reinforced Coupled |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 - 120 °C | 243 - 248 °F | |
C.O.I.M. EXTER S® S 402 Isophthalic Resin Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 402: High-quality re.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | ASTM D648 |
Aclo Accutech Polypropylene Copolymer CP0436T30L1 Talc Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPHC T11030 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPHC TS20040 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | ASTM D648 |
Samyang Triel® 5650 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5650 is an extrusion grade.Information provided by Samyang. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 117 °C | 243 °F | ASTM D648 |
Samyang Triel® 5652EM Thermoplastics Polyetherester Elastomer, Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5652EM is an extrusion grade.Information provided by Samyang. |