Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | Unannealed; ASTM D648 |
Multibase Multi-Pro® 4012 TH Polypropylene Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Lawn and Garden EquipmentTable ProductsFurnitureInformation provided by Multibase |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | ASTM D648 |
RheTech Products HP517-00 23% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trim moldingsSill platesTire coverInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | ASTM D648 |
RheTech Products M40P200-01 40% Mica Reinforced Polypropylene Copolymer, Black Applications: Automotive applicationsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | ASTM D648 |
RheTech Products T10P100-00 10% Talc Reinforced Polypropylene, Natural Applications: Consumer goodsIP structural componentsInterior trimInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | ASTM D648 |
RheTech Products T10P100-01 10% Talc Reinforced Polypropylene, Black Applications: Consumer goodsAir ductsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | ASTM D648 |
RheTech Products T40P200-01 40% Talc Reinforced Polypropylene Copolymer, Black Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | ASTM D648 |
RheTech Products T40P250-00 40% Talc Reinforced Polypropylene Copolymer, Natural Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | ASTM D648 |
Ineos N01N-00 Polypropylene Impact Copolymer Grade N01N-00 is a high stiffness, impact copolymer specially designed for freezer-to-microwave performance. This extrusion grade resin exhibits an excellent balance of impact and stiffness properti.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PC/PBT IM 1702 BK Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PC/PBT IM 1799 BK Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PC/PBT IM 5720 A BK Availability: North AmericaForms: PelletsAdditive: Impact Modifier and UV StabilizerFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PC/PBT IM 5727 BK Availability: North AmericaForms: PelletsAdditive: Impact Modifier and UV StabilizerFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PC/PBT IM 6120 BK Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PC/PBT IM 6200 BK Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PC/PBT IM 6600 Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1200 Calcium Carbonate-Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1200 is a 40% calcium carbonate-filled homopolymer polypropylene. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | ASTM D648 |
Washington Penn Homopolymer Polypropylene 20% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1427 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1247 is a 25% mineral filled copolymer polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1200 Calcium Carbonate-Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1200 is a 40% calcium carbonate-filled homopolymer polypropylene. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1427 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1247 is a 25% mineral filled copolymer polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1200 Calcium Carbonate-Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1200 is a 40% calcium carbonate-filled homopolymer polypropylene. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1427 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1247 is a 25% mineral filled copolymer polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | ASTM D648 |
Lubrizol ESTALOC® 59600 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation pro.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | ASTM-D648 |
CTC X-PRO TF 1113 HP Polypropylene Homopolymer, 13% Talc Filled X-PRO TF 1113 HP is a 13% talc reinforced polypropylene homopolymer, heat stabilized, and made of 98% recycled content. It has applications in: automotive under hood, IP components, fan and lightin.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | ASTM-D648 |
CTC X-PRO TF 1120 HP Polypropylene Homopolymer, 20% Talc Filled X-PRO TF 1120 HP is a 20% talc reinforced polypropylene homopolymer, heat stabilized, and made of 98% recycled content. It has applications in: automotive under hood, IP components, fan and lightin.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | |
Aaron Industries AAROPRENE® AE PC/ABS 7000-2 PC/ABS Engineered Resin Melt flow index may be specified. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | ASTM D648 |
Plastics Group Polifil® T-10 10% Talc-Reinforced Polypropylene Polifil® T series compounds are homopolymer polypropylene resins reinforced with asbestos-free talc. They possess high flex modulus, high deflection temperature, good chemical resistance and colora.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1200 Calcium Carbonate-Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1200 is a 40% calcium carbonate-filled homopolymer polypropylene. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® ABS CF40 BK 40% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 40% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 118 °C | 245 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1427 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1247 is a 25% mineral filled copolymer polypropylene.Information provided by A. Schulman. |