Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 135 - 140 °C
275 - 284 °F
ASTM D1525, HDT Method B
Loxim 100 00V0 Polycarbonate, Flame Retardant
Information provided by Loxim Industries
Deflection Temperature at 0.46 MPa (66 psi) 135 - 140 °C
275 - 284 °F
ASTM D1525, HDT Method B
Loxim 100 00V2 Polycarbonate, Flame Retardant
Information provided by Loxim Industries
Deflection Temperature at 0.46 MPa (66 psi) 125 - 140 °C
257 - 284 °F
CPC - Vycom FLAMETEC™ KYTEC® PVDF
Kytec® PVDF, the homopolymer of 1, 1-difluoroethene, is a tough engineering thermoplastic that offers a unique balance of properties. Kytec has the characteristic stability of fluoropolymers when e..
Deflection Temperature at 0.46 MPa (66 psi) 135 - 140 °C
275 - 284 °F
C.O.I.M. EXTER S® S 200 Special Laminate
Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 200: Tack-free and h..
Deflection Temperature at 0.46 MPa (66 psi) 125 - 140 °C
257 - 284 °F
ASTM D648
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Deflection Temperature at 0.46 MPa (66 psi) 125 - 140 °C
257 - 284 °F
ASTM D648
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli..
Deflection Temperature at 0.46 MPa (66 psi) 125 - 140 °C
257 - 284 °F
ASTM D648
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Deflection Temperature at 0.46 MPa (66 psi) 125 - 140 °C
257 - 284 °F
ASTM D648
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha..
Deflection Temperature at 0.46 MPa (66 psi) 125 - 140 °C
257 - 284 °F
ASTM D648
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Deflection Temperature at 0.46 MPa (66 psi) 112 - 140 °C
234 - 284 °F
ASTM D648
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
Deflection Temperature at 0.46 MPa (66 psi) 112 - 140 °C
234 - 284 °F
ASTM D648
Arkema Group KYNAR® 460 Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Broad molecular weight distribution, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, ..
Deflection Temperature at 0.46 MPa (66 psi) 125 - 140 °C
257 - 284 °F
ASTM D648
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..