Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 150 °C | 302 °F | Unannealed; ISO 75-2/B |
PolyOne Trilliant™ HC HC6200-5002 XR Grey Polyamide 12 (Nylon 12) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 150 °C | 302 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPH GF5030 PB Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 150 °C | 302 °F | ISO 75-1/-2 |
DuPont Performance Polymers Crastin® S600F40 BK851 PBT
(Unverified Data**) Crastin® S600F40 BK851 is an unreinforced, lubricated, low viscosity, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 150 °C | 302 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPH MGF5040 Polypropylene Homopolymer, Multifiller Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 150 °C | 302 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS (Europe-Africa-Middle East) Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 150 °C @Thickness 3.20 mm |
302 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Valox® HX215HP PBT High Flow, Unreinforced, Polybutylene Terephthalate (PBT). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food conta.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 150 °C | 302 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PBT 613 RD Availability: North AmericaForms: PelletsUL File Number: E157318Appearance: Red8661111Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 150 °C @Thickness 3.20 mm |
302 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON DE0039 PC (Asia Pacific) LNP* Stat-kon* DE0039 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Flame Retardant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 150 °C | 302 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP 5E003M FP-V (PVDF) LNP* THERMOCOMP* 5E003M is a compound based on PVDF resin containing 15% Milled Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 150 °C | 302 °F | Unannealed; ASTM D648 |
Teknor Apex Sinpolene GPP5620 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Glass Fiber Reinforcement, 20% Filler by Weight Features: Good Dimensional Stability; High Heat Resistance; .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 150 °C | 302 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1285U Glass Filled, UV Stable Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1285U is a 20% glass filled UV stable impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 150 °C | 302 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1080 Glass Fiber-Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1080 is a 20% fiber-reinforced homopolymer polypropylene with excellent strength and heat resistance. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 150 °C | 302 °F | |
Polyplastics TOPAS® 6015 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade) A similar grade to 6013. However, heat deflection temperature is (HDT/B) = 150°C. This is a temperature that cannot be achieved with many other amorphous polymers.Information provided by PolyPlasti.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 150 °C | 302 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1285U Glass Filled, UV Stable Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1285U is a 20% glass filled UV stable impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 150 °C | 302 °F | DIN 53461 |
Polyram RamOfin PPH307G6 Polypropylene, 30% Glass Fiber 30% glass fiber reinforced, impact modified polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 150 °C | 302 °F | ISO 75 |
Polyram RamOfin PPH308G50 Polypropylene, 50% Glass Fiber, Impact Modified 50% Glass fiber reinforced, heat stabilized, impact modified polypropylene for injection molding applications.Information provided by Polyram. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 150 °C | 302 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1285U Glass Filled, UV Stable Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1285U is a 20% glass filled UV stable impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 150 °C | 302 °F | ISO 179 |
CP-Polymer-Technik Wellamid® 6600/508 HWUVCP Nylon 66, Impact Modified, UV Stabilized, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 150 °C | 302 °F | ISO 75-1/-2 |
DuPont Performance Polymers Crastin® S600LF NC010 PBT Crastin® S600LF NC010 is an unreinforced, Teflon® PTFE powder lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 150 °C | 302 °F | ASTM D648 |
E-Polymers TEKAPPO® JF2 Un-Reinforced Heat Resistant Chemical Resistance M-PPO Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 150 °C | 302 °F | DIN EN ISO 75-2/Be |
BASF Elastollan R 2005/1 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 150 °C | 302 °F | ISO 75 |
BASF Ultraform N 2320 U017 UNC Q600 POM Ultraform N 2320 U017 UNC Q600 is a UV stabilized rapidly freezing injection-molding POM grade. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 150 °C | 302 °F | ASTM D648 |
Samyang Trirex® 3025GRU30 Polycarbonate, 30% Glass Reinforced TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, electr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 150 °C | 302 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics NORYL PX1786G PPE+HIPS (Europe-Africa-Middle East) NORYL PX1786G is a 30 % glass filled material with a Vicat B/120 of 160 °C. |