Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 442 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 228 °C
442 °F
ASTM D648
Nilit Polynil® P50FL Externally Lubricated, Lightly Nucleated Nylon 66
Description: Polynil P50FL is a general purpose injection molding grade that is widely used for gears, bearings, fasteners, clips.Key characteristics: Excellent flowGood toughnessGood overall mechan..
Deflection Temperature at 0.46 MPa (66 psi) 228 °C
442 °F
ASTM D648
Nilit Polynil® P60 Medium Viscosity Nylon 66
Description: Polynil P60 is a grade has a viscosity that has been optimized for monofilament extrusion.Key characteristics: Viscosity number 155 gr/cm3Excellent melt stabilityHigh elongationInformat..
Deflection Temperature at 0.46 MPa (66 psi) 228 °C
442 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP LUBRICOMP RX85514 PA 66
LNP LUBRICOMP* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated.
Deflection Temperature at 0.46 MPa (66 psi) 228 °C
442 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP LUBRICOMP RX88514 PA 66
LNP LUBRICOMP* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). AddedLNP LUBRICOMP* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). A..
Deflection Temperature at 0.46 MPa (66 psi) 228 °C
442 °F
ASTM D648
Cheng Yu Plastic N6GV20 Flame Retardant Nylon 6, 20% Glass Filled
Deflection Temperature at 0.46 MPa (66 psi) 228 °C
442 °F
ASTM D648
Cheng Yu Plastic T885GV3 Flame Retardant PBT, 30% Glass Fiber
Deflection Temperature at 0.46 MPa (66 psi) 228 °C
442 °F
ASTM D648
Cheng Yu Plastic T890G3 PBT, 30% Glass Fiber
Deflection Temperature at 0.46 MPa (66 psi) 228 °C
442 °F
ASTM D648
E-Polymers TEKAMID® TA210IR Impact Modified PA66 Resin
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.T-series: Impact modified,..