Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 500 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 210 - 260 °C
410 - 500 °F
Average value: 219 °C Grade Count:15
Overview of materials for Nylon 6, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a..
Deflection Temperature at 0.46 MPa (66 psi) 190 - 260 °C
374 - 500 °F
Average value: 230 °C Grade Count:56
Overview of materials for Nylon 66, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
Deflection Temperature at 0.46 MPa (66 psi) 220 - 260 °C
428 - 500 °F
Average value: 255 °C Grade Count:20
Overview of materials for Nylon 66, 60% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. ..
Deflection Temperature at 0.46 MPa (66 psi) 210 - 260 °C
410 - 500 °F
Average value: 247 °C Grade Count:13
Overview of materials for Nylon 66, 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc..
Deflection Temperature at 0.46 MPa (66 psi) 240 - 260 °C
464 - 500 °F
Average value: 253 °C Grade Count:15
Overview of materials for Nylon 66, 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in..
Deflection Temperature at 0.46 MPa (66 psi) 240 - 260 °C
464 - 500 °F
Average value: 257 °C Grade Count:14
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
Deflection Temperature at 0.46 MPa (66 psi) 124 - 260 °C
255 - 500 °F
Average value: 231 °C Grade Count:54
Overview of materials for Nylon 66, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu..
Deflection Temperature at 0.46 MPa (66 psi) 188 - 260 °C
370 - 500 °F
Average value: 234 °C Grade Count:10
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi..
Deflection Temperature at 0.46 MPa (66 psi) 85.0 - 260 °C
185 - 500 °F
Average value: 192 °C Grade Count:11
Overview of materials for Nylon 6-3
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Deflection Temperature at 0.46 MPa (66 psi) 155 - 260 °C
311 - 500 °F
Average value: 223 °C Grade Count:50
Overview of materials for Nylon 66, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
Deflection Temperature at 0.46 MPa (66 psi) 240 - 260 °C
464 - 500 °F
Average value: 255 °C Grade Count:6
Overview of materials for Nylon 66, 40% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Carbon Fiber Filled". Specific grades with carbon fiber content between 35% and 44% are in..
Deflection Temperature at 0.46 MPa (66 psi) 110 - 260 °C
230 - 500 °F
Average value: 198 °C Grade Count:17
Overview of materials for Nylon 6, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria..