Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM D648 |
RheTech Products FT7012-707UV Thermoplastic Polyolefin, UV Stabilized, 848 Black Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | Unannealed; ASTM D648 |
Phillips 66 COPYLENE® CR020CL Polypropylene Impact Copolymer COPYLENE® CR020CL is a random copolymer formulated with advanced clarifier technology and with antistat and is specially designed to excel in extrusion blowmolding processes. EBM bottles will have .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM D648 |
M. Holland Company CP510 Polypropylene Copolymer Additives: Heat Stabilizer, Nucleating AgentsFeatures: High Flow, High Impact Resistance, Heat Stabilizer, NucleatedUses: Construction Applications, Lawn and Garden EquipmentApprovals: FDA 21 CFR 17.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM D648 |
Garland Manufacturing GAR-DUR® Ultra High Molecular Weight Polyethylene (UHMW-PE) GAR-DUR® plastic parts are made from ultra high molecular weight (UHMW) polymer having a molecular weight of 4.2 million and greater. Garland Manufacturing Company has been processing UHMW resin .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM D648 |
LG Chemical SEETEC T3410 Polypropylene Random Terpolymer Features: Seetec T3410 is a polypropylene-ethylene-butene random terpolymer designed for the production of Transparent Film and Expandable PP for low seal temperature and high impact strength. It of.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C @Thickness 6.40 mm |
176 °F @Thickness 0.252 in |
ASTM D648 |
Kingfa NH-627 Flame Retardant ABS Features:UL 94 V-2 @ 1.6mmHalogen-free flame retardantHigh flowApplications:OA deviceDigital cameraVidiconInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C @Thickness 3.20 mm |
176 °F @Thickness 0.126 in |
Unannealed; ASTM D648 |
LG Chemical LUPOL HI5302S PP+MF15%, High Impact Description: Injection Molding, PP+MF15%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsInformation provided by LG Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Noryl V180HF PPE+HIPS (Europe-Africa-Middle East) NORYL V180HF is an unfilled, flame retardant material. It has been fully optimized w.r.t. flow and is halogen free according to VDE/DIN 472 part 815.This data was supplied by SABIC-IP for the Europe.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | GOST 12021 |
Sibur H250 GP Polypropylene Homopolymer Polypropylene homopolymer with narrow molecular weight distribution. It features high fluidity, an optimal stabilization package and balanced physical and mechanical properties.general purpose produ.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM D648 |
A. Schulman SUPERLINEAR™ XL 0370 Rotational Molding Resin DescriptionSuperlinear XL 0370 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ISO 75-2 |
Borealis HH450MO Polypropylene HH450MO is a polypropylene homopolymer intended for injection molding. This grade is especially suitable for high-speed injection molding of articles demanding easy flow. This polymer is a CR (cont.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM D648 |
A. Schulman PP 1407H-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1407H-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 1407H-01 meets FDA Regulation 21 CFR 177.1520 for food contact .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM D648 |
A. Schulman PP 3457-01 Copolymer Polypropylene DescriptionPolypropylene PP 3457-01 is a copolymer polypropylene combining high impact at cold temperatures while maintaining stiffness. Ideal for durables in such applications for the furniture, a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM D648 |
A. Schulman PP 3457-01 Copolymer Polypropylene DescriptionPolypropylene PP 3457-01 is a copolymer polypropylene combining high impact at cold temperatures while maintaining stiffness. Ideal for durables in such applications for the furniture, a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | DIN 53461 |
Polyram PlusTek PA830 Nylon 6.6, Impact Modified Impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | DIN 53461 |
Polyram PlusTek PA860 Nylon 6.6, Impact Modified Super tough - impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM D648 |
A. Schulman PP 1404-01 Polypropylene High Impact Polypropylene DescriptionPolypropylene PP 1404-01 is a medium flow, high-impact polypropylene for injection molded parts. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM D648 |
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM D648 |
A. Schulman PP 3457-01 Copolymer Polypropylene DescriptionPolypropylene PP 3457-01 is a copolymer polypropylene combining high impact at cold temperatures while maintaining stiffness. Ideal for durables in such applications for the furniture, a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM D648 |
A. Schulman PP 3457-01 Copolymer Polypropylene DescriptionPolypropylene PP 3457-01 is a copolymer polypropylene combining high impact at cold temperatures while maintaining stiffness. Ideal for durables in such applications for the furniture, a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM D648 |
Covestro Baydur® 730 IBS Polyurethane Structural Foam RIM, Density 40 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ISO 75-1/-2 |
DSM Arnitel® UM552 Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM-D648 |
CTC X-PRO CTC PP1050 Polypropylene Homopolymer X-PRO PP 1050 is a polypropylene homopolymer. Its applications are: general purpose industrial injection molding, virgin polypropylene diluents, and polymer base for glass, talc or specialty filled.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ISO 75-1/-2 |
DSM Arnitel® UM552 55 Shore D Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ISO R75 |
Arkema Group Orgalloy® LE60 THM Polyamide Alloy Polyamide Alloy, Semi-Flexible gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | |
C.O.I.M. EXTER S® S 203 Special Laminate Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 203: Polyester resin.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ISO 75 |
Polyram RamLloy PVB702 Nylon/ABS Alloy, Impact Modified Impact modified, UV stabilized Nylon/ABS alloy for injection molding applications.Information provided by Polyram. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM D648 |
A. Schulman POLYFLAM™ RPP 1221 Low-Blooming, General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in. Informati.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ISO 75-2 |
Borealis Bormed™ HE2581-PH HDPE for Healthcare Applications Bormed HE2581-PH is a high-density polyethylene intended for blow molding of products with high stiffness and very good environmental stress crack resistance (ESCR). Bormed HE2581-PH can as well be .. |