Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® BFL2010 PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC with improved flow. Available in opaque colors. |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® BFL2015 PC (Europe-Africa-Middle East) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® EM3110 PC (Asia Pacific) Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses. |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® FL913 PC Various weight reduction at 0.250"" (6.35 mm) wall. 10% GR, high flexural strength/modulus. UL rated V-0/5VA (all except natural). UV-stabilized. |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® FXE4271L PC (Asia Pacific) Lexan* FXE4271L is a 10% glass filled, impact modified polycarbonate with excellent light-shield capability. It is designed for high flow, superior surface appearance, enhance release and good impac.. |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® HFD4413 PC Lexan* HFD4413 is a 30% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® HFD4413 PC (Asia Pacific) Lexan* HFD4413 is a 30% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® HP9NR PC Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. For blow molding .. |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® BFL2000U PC (Europe-Africa-Middle East) Lexan* BFL2000U Polycarbonat (PC) resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating. Lexan* BFL2000U is designed for hig.. |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | |
PTS Tristar® PC-10GFR 10% Glass Reinforced Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® FL2003 PC (Asia Pacific) Various weight reductions at 0.250" (6.35mm) wall. Low temperature impact and high heat resistant. Excellent surface. UV-stabilized.This data was supplied by SABIC-IP for the Asia Pacific region... |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® FL405 PC Various weight reductions at 0.250"" (6.38 mm) wall. Impact resistant, superior processing, excellent surface. UL94 V-0 at 0.120 |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® FL410 PC Various weight reductions at 0.250: (6.38 mm) wall. Thin wall capability high flexural mod, strength and creep resistant. V-0/5V - 0.157""(3.98 mm). |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® HFD4211 PC (Europe-Africa-Middle East) Lexan* HFD4211 is a 10% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® HFD4472 PC Lexan* HFD4472 is a 20% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4472 has enhanced mold release, impact ductili.. |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® ML3041 PC (Europe-Africa-Middle East) LEXAN ML3041 has been developed for the injection moulding of thin-wall, complex parts that require high mechanical properties and impact resistance.This data was supplied by SABIC-IP for the Europe.. |
|||
UL RTI, Electrical | 80.0 °C @Thickness >=3.00 mm |
176 °F @Thickness >=0.118 in |
|
LG Chemical LUCON CP2100-KA02 PC+CF Description Injection Molding Grade, PC+CF, Electrostatic Dissipation, Low Surface ResistanceApplication: LCD Tray, HDD BracketCAS No. 103598-77-2 and 7440-44-0Information provided by LG Chemical |
|||
UL RTI, Electrical | 80.0 °C @Thickness 0.500 - 2.50 mm |
176 °F @Thickness 0.0197 - 0.0984 in |
|
LG Chemical Lupoy 3010-10 Polycarbonate Resin Description: LUPOY PC 3010-10 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
UL RTI, Electrical | 80.0 °C @Thickness 0.500 - 2.50 mm |
176 °F @Thickness 0.0197 - 0.0984 in |
|
LG Chemical Lupoy 3030-10 Polycarbonate Resin Description: LUPOY PC 3030-10 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | |
LG Chemical LUPOY GN5001RFT PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Good FlowApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical.. |
|||
UL RTI, Electrical | 80.0 °C @Thickness >=0.700 mm |
176 °F @Thickness >=0.0276 in |
|
LG Chemical LUPOY SC1004L PC, High Impact Description: Injection Molding, PC, General Purpose, High Flow, High Impact, Chemical ResistanceApplication: Mobile Phone HousingInformation provided by LG Chemical |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | |
LG Chemical LUPOY SG5009FA PC/ABS/PMMA, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High Gloss, Anti-scratchApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9, 9011-14-7 and 181028-79-5Informatio.. |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics LNP STAT-KON DX89795 PC (Europe-Africa-Middle East) LNP* STATKON* DX89795 is a compound based on Polycarbone resin containing Carbon Powder. Added features include: Electrically Conductive, Easy Molding, Mold Release. |
|||
UL RTI, Electrical | 80.0 °C @Thickness 1.47 mm |
176 °F @Thickness 0.0579 in |
UL 746B |
Teijin Panlite® BS-8120R Friction and Abrasion Resistant, Carbon Fiber Reinforced Polycarbonate Resin CF 20% reinforced grade, meeting UL 94 V-2. it is compounded with fluorine powder to improve friction and abrasion resistance and also exhibits a mold release property, maintaining excellent charact.. |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics NORYL GN390 PPE+PS (Asia Pacific) Closed loop recycle grade for CANON, 13% PCR-PS loaded, HDT 90C, V-0/1.2mm |
|||
UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
Covestro Makrolon® FR6901 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Hig.. |
|||
UL RTI, Electrical | 80.0 °C @Thickness 1.50 mm |
176 °F @Thickness 0.0591 in |
UL 746B |
Diamond Polymers ABS 2512 Description: Injection Molding Grade, Medium Impact, High FlowInformation provided by Diamond Polymers, Inc. |
|||
UL RTI, Electrical | 80.0 °C @Thickness 1.50 mm |
176 °F @Thickness 0.0591 in |
UL 746B |
Diamond Polymers ABS 7602B Description: Blow Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
UL RTI, Electrical | 80.0 °C @Thickness 5.99 mm |
176 °F @Thickness 0.236 in |
UL 746 |
Polymer Resources PCSF-FR1 Polycarbonate, 10% Glass Reinforced Structural Foam Grade Polycarbonate, 10% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing con.. |
|||
UL RTI, Electrical | 80.0 °C @Thickness >=0.700 mm |
176 °F @Thickness >=0.0276 in |
|
LG Chemical LUPOY SC1004ML PC, High Impact Description: Injection Molding, PC, General Purpose, High Impact, Good Coloring, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9046-16-6Information provided by LG Chemical.. |