Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -48.0 °C | -54.4 °F | Base Oil; ASTM D97 |
Nye Lubricants 186 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -48.0 °C | -54.4 °F | Base Oil; ASTM D97 |
Nye Lubricants 186B (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -48.0 °C | -54.4 °F | Base Oil; ASTM D97 |
Nye Lubricants 186C (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -48.0 °C | -54.4 °F | Base Oil; ASTM D97 |
Nye Lubricants 374A (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -48.0 °C | -54.4 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8520 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -48.0 °C | -54.4 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8521 (841-1) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -48.0 °C | -54.4 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8521BL (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -48.0 °C | -54.4 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8521R (841RP-1) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -48.0 °C | -54.4 °F | Base Oil; ASTM D97 |
Nye Lubricants 789DMF (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -48.0 °C | -54.4 °F | ASTM D97 |
ExxonMobil 12M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Pour Point | -48.0 °C | -54.4 °F | ASTM D97 |
ExxonMobil Mobil Delvac 50 Synthetic Transmission Fluid Mobil Delvac Synthetic Transmission Fluid 50 is a fully synthetic, manual transmission lubricant engineered to meet the most demanding extended drain and OEM warranty requirements. It is recommended.. |
|||
Pour Point | -48.0 °C | -54.4 °F | ASTM D97 |
ExxonMobil Mobil Delvac 75W-90 Synthetic Gear Oil Mobil Delvac Synthetic Gear Oil 75W-90 and 80W-140 are synthetic drivetrain lubricants engineered to meet the most demanding extended drain and warranty requirements. These products are designed for.. |
|||
Pour Point | -48.0 °C | -54.4 °F | ASTM D97 |
ChevronTexaco Clarity® ISO 150 Synthetic Paper Machine Oil FeaturesChevron Clarity Synthetic Paper Machine Oils combine the unique ashless formulation of Chevron Clarity® Paper Machine Oils with the superior performance properties of polyalphaolefin (PAO) .. |
|||
Pour Point | -48.0 °C | -54.4 °F | |
ChevronTexaco Heavy Duty Synthetic Automatic Transmission Fluid Texaco Synthetic Automatic Transmission Fluid Heavy Duty delivers value through:Extended drains of up to four times that of a conventional automatic transmission fluid.Protection against the formati.. |
|||
Pour Point | -48.0 °C | -54.4 °F | ASTM D97 |
ChevronTexaco Mechanism LPS® ISO 32 Hydraulic Oil Chevron Mechanism LPS Hydraulic Oils are highly refined, paraffinic oils containing oxidation and rust inhibitors, and special antiwear additives to extend the life of hydraulic pumps and motor part.. |
|||
Pour Point | -48.0 °C | -54.4 °F | ASTM D97 |
ChevronTexaco RPM® SAE 75W-90 Synthetic Gear Lubricant FeaturesChevron RPM Synthetic Gear Lubricant is a heavy duty, extreme pressure, multigrade automotive gear lubricant.It is manufactured from synthesized hydrocarbon base fluids which have excellent .. |
|||
Pour Point | -48.0 °C | -54.4 °F | |
ChevronTexaco Syn-Star® GL SAE 75W-90 Texaco Syn-Star GL oils deliver value through:Excellent thermal and oxidation stability — The synthetic hydrocarbon base oil used in these products provides outstanding stability.Extended drain cap.. |
|||
Pour Point | -48.0 °C | -54.4 °F | |
ChevronTexaco Syn-Star® TL SAE 50 Texaco Syn-Star® TL delivers value through:Excellent thermal and oxidation stability — The synthetic hydrocarbon base oil used in this product provides outstanding stability.Extended drain capabil.. |
|||
Pour Point | -48.0 °C | -54.4 °F | ASTM D97 |
ChevronTexaco THF W FeaturesChevron THF W is a high quality, multifunctional fluid, specially formulated for low temperature use in transmissions, final drives, wet brakes, and hydraulic systems of tractors and other e.. |
|||
Pour Point | -48.0 °C | -54.4 °F | ASTM D97 |
ExxonMobil 150 Mobilgear SHC XMP Series Mobilgear SHC XMP Series supreme performance, fully synthetic industrial gear oils designed to provide optimum equipment protection and oil life even under extreme conditions. Mobil polyalphaolefin .. |
|||
Pour Point | -48.0 °C | -54.4 °F | ASTM D97 |
ExxonMobil 32 Mobil EAL Arctic Series Mobil EAL Arctic Series are high performance Environmental Awareness Lubricants (EAL) that are fully synthetic products designed specifically for the lubrication of refrigeration compressors and sys.. |
|||
Pour Point | -48.0 °C | -54.4 °F | ASTM D97 |
ExxonMobil 625 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are .. |
|||
Pour Point | -48.0 °C | -54.4 °F | ASTM D97 |
ExxonMobil 626 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are .. |
|||
Pour Point | -48.0 °C | -54.4 °F | ASTM D97 |
ExxonMobil Mobil Delvac 50 Synthetic Transmission Fluid Mobil Delvac Synthetic Transmission Fluid 50 is a fully synthetic, manual transmission lubricant engineered to meet the most demanding extended drain and OEM warranty requirements. It is recommended.. |
|||
Pour Point | -48.0 °C | -54.4 °F | ASTM D97 |
ChevronTexaco Clarity® ISO 100 Synthetic Paper Machine Oil FeaturesChevron Clarity Synthetic Paper Machine Oils combine the unique ashless formulation of Chevron Clarity® Paper Machine Oils with the superior performance properties of polyalphaolefin (PAO) .. |
|||
Pour Point | -48.0 °C | -54.4 °F | |
ChevronTexaco Havoline® ATF+3® Automatic Transmission Fluid Havoline Automatic Transmission Fluid ATF+3 delivers value through:Correct viscosity and frictional characteristics to ensure smooth operation in Chrysler transmissions.Long-lasting viscosity modifi.. |
|||
Pour Point | <= -48.0 °C | <= -54.4 °F | ASTM D97 |
ExxonMobil Mobil Pegasus 1 40 Mobil Pegasus 1 is a high performance synthetic gas engine oil designed to meet the highest performance requirements of the most demanding naturally aspirated and turbocharged stoichiometric and lea.. |
|||
Pour Point | -48.0 °C | -54.4 °F | ASTM D97 |
ExxonMobil 625 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are .. |
|||
Pour Point | -48.0 °C | -54.4 °F | ASTM D97 |
ExxonMobil 626 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are .. |