Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS (Asia Pacific) Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes.. |
|||
Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is RoHS compliant and halogen free acc.. |
|||
Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® 945AU PC Lexan* 945AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a V0 UL rating and is UV stabilized, providing additiona.. |
|||
Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® CFR9111 PC COPOLYMER (Europe-Africa-Middle East) Lexan* CFR9111 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm and good flow capability. .. |
|||
Glow Wire Test | 850 °C @Thickness 0.800 mm |
1560 °F @Thickness 0.0315 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent .. |
|||
Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer (Asia Pacific) Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
Glow Wire Test | 850 °C @Thickness 1.00 mm |
1560 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® EXL8134 PC COPOLYMER (Asia Pacific) Lexan* EXL8134 is a PC/siloxane copolymer resin with high flow, excellent low temperature impact and 30% post consumer recycle content. Limited availability and restricted color only. Higher color v.. |
|||
Glow Wire Test | 850 °C @Thickness 1.00 mm |
1560 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® HPS2 PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable.. |
|||
Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer (Asia Pacific) Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Glow Wire Test | 850 °C @Thickness 1.00 mm |
1560 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® LUX2180T_ PC (Europe-Africa-Middle East) Global grade. LEXAN LUX2180T is an injection moulding grade especially designed for manufacturing optical parts requiring easy flow properties combined with very high transmission and color stabilit.. |
|||
Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® LUX9132C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX9132C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
SABIC Innovative Plastics LNP KONDUIT PX11311 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 FR compound |
|||
Glow Wire Test | 850 °C @Thickness 1.00 mm |
1560 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® 221R PC (Europe-Africa-Middle East) LEXAN 221R is a low viscosity multi purpose grade and contains a release agent to ensure easy processing. This grade is UL94-V2 at 0.4 mm approved. |
|||
Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® 925AU PC Lexan* 925AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing addit.. |
|||
Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® 945A PC Lexan* 945A Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and ti.. |
|||
Glow Wire Test | 850 °C @Thickness 1.00 mm |
1560 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® EX1632T PC (Europe-Africa-Middle East) LEXAN* EX1632T polycarbonate resin, MVR (300C/1.2kg) 6 cm3/10min, high viscosity, branched, extrusion, mold release, UV stabilized, transparent, translucent and opaque colors. Multiwall sheet, Profi.. |
|||
Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer (Asia Pacific) Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Glow Wire Test | 850 °C @Thickness 2.00 mm, Time 5.00 sec |
1560 °F @Thickness 0.0787 in, Time 0.00139 hour |
IEC 695-2-1 |
LG Chemical Lupoy 1300-15 Polycarbonate Resin Description: LUPOY PC 1300-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Glow Wire Test | 850 °C @Thickness 2.00 mm, Time 5.00 sec |
1560 °F @Thickness 0.0787 in, Time 0.00139 hour |
IEC 695-2-1 |
LG Chemical Lupoy 1261-03 Polycarbonate Resin Description: LUPOY PC 1261-03 resin is designed for extrusion blow molding(EBM) and injection stretch blow molding (ISBM) products. It exhibits an excellent physical property balance of heat resista.. |
|||
Glow Wire Test | 850 °C @Thickness 2.00 mm, Time 5.00 sec |
1560 °F @Thickness 0.0787 in, Time 0.00139 hour |
IEC 695-2-1 |
LG Chemical Lupoy 1301V-7 Polycarbonate Resin Description: LUPOY PC 1301V-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.. |
|||
Glow Wire Test | 850 °C @Thickness 2.00 mm, Time 5.00 sec |
1560 °F @Thickness 0.0787 in, Time 0.00139 hour |
IEC 695-2-1 |
LG Chemical Lupoy 1201-22 Polycarbonate Resin Description: LUPOY PC 1201-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Glow Wire Test | 850 °C @Thickness 3.00 mm |
1560 °F @Thickness 0.118 in |
IEC 60695-2-12 |
SABIC Innovative Plastics NORYL WCD891B PPE-TPE (Europe-Africa-Middle East) Non-halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications. Strong flame retardant performance capable of meeting VW-1 and 80°C end use tempera.. |
|||
Glow Wire Test | 850 °C @Thickness 3.00 mm |
1560 °F @Thickness 0.118 in |
IEC 60695-2-12 |
SABIC Innovative Plastics NORYL WCP781 PPE-TPE (Europe-Africa-Middle East) Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto.. |
|||
Glow Wire Test | 850 °C @Thickness 3.00 mm |
1560 °F @Thickness 0.118 in |
IEC 60695-2-12 |
SABIC Innovative Plastics NORYL WCP921 PPE-TPE (Europe-Africa-Middle East) Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain relief.. |
|||
Glow Wire Test | 850 °C @Thickness 3.20 mm |
1560 °F @Thickness 0.126 in |
IEC 60695-2-12 |
SABIC Innovative Plastics NORYL GFN3V PPE+HIPS (Europe-Africa-Middle East) NORYL GFN3V is a 30 % glass fibre reinforced material with a HDT/A of 145C according ISO 75. NORYL GFN3V has been approved for potable water applications up to 85C by the UK WFBS according BS 6920 i.. |
|||
Glow Wire Test | 850 °C | 1560 °F | GWFI; IEC 60695-2-12 |
Covestro Apec® 1603 High-Heat Polycarbonate This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along.. |
|||
Glow Wire Test | 850 °C @Thickness 1.00 mm |
1560 °F @Thickness 0.0394 in |
Glow Wire Ignition Temperature GWIT; IEC 60695-2-13 |
DSM Arnitel® EL740 74 Shore D, Injection Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Glow Wire Test | 850 °C | 1560 °F | < 30 sec; GB/2099.1 |
Zhejiang Juner PC-A1-9 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Glow Wire Test | 850 °C @Thickness 1.00 mm |
1560 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® ML144R PC (Europe-Africa-Middle East) Medium viscosity, multi purpose polycarbonate resin with added release agent. Food contact approved in limited colors. Effective January 15th, 2007 this grade will no longer be supported with bioc.. |