Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 50.0 °C @Thickness 1.50 mm |
122 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Hytrel® 4069 TPC-ET
(Unverified Data**) Hytrel® 4069 is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injection.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness 3.00 mm |
122 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Hytrel® 4069 TPC-ET
(Unverified Data**) Hytrel® 4069 is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injection.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness 1.50 mm |
122 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Delrin® 150 NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has excellent thermal stability, low die deposit, and enhanced crystallization for low porosity.Information pr.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness 0.750 mm |
122 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness 0.750 mm |
122 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Delrin® 500CL BK601 Acetal Homopolymer
(Unverified Data**) Delrin® 500CL BK601 is a medium viscosity acetal homopolymer containing a chemical lubricant, designed for low wear and friction against metals.Information provided by DuPont Performance Polymers |
|||
UL RTI, Electrical | 50.0 °C @Thickness 0.800 mm |
122 °F @Thickness 0.0315 in |
UL 746B |
DuPont Performance Polymers Delrin® 988PA NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 988PA NC010 is a low viscosity acetal homopolymer for injection molding with low screw deposit. It is especially formulated for gear applications requiring high precision and dimensional st.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical GPPS 25SP(E) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=1.60 mm |
122 °F @Thickness >=0.0630 in |
|
LG Chemical HIPS 403AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 21850-44-2 and 1309-64-4Information provided by LG Chemical |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical HIPS 406AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical HIPS 410AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=3.20 mm |
122 °F @Thickness >=0.126 in |
|
LG Chemical HIPS 460AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 25713-60-4, 84852-53-9 and 1309-64-4Information provided by LG Chemical |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical HIPS 501S PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: Refrigerator Food Holder, Food Container, Plastic Toy, Sheet or Film of Yot ReceptacleCAS: 9003-55-8Information provi.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical HIPS MI730 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical HIPS MI750L PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical HIPS MI770 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical KEYFLEX BT 1040D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical KEYFLEX BT 1055D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical LI911 ASA Description: Good Weatherability, High FlowApplication: Air-conditioner grill, Sawing Machine Cover, Electric/Electronic ApplicationsCAS: 26299-47-8Information provided by LG Chemical |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical LUMAX HR5157 PBT+ABS+GF15%, Heat Resistance Description: Injection Molding Grade, PBT+ABS+GF15%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical |
|||
UL RTI, Electrical | 50.0 °C @Thickness 1.50 mm |
122 °F @Thickness 0.0591 in |
|
Aardvark Polymers AARTEL® 2100UV Acetal Homopolymer Rotational Molding Resin Aartel 2100UV is a natural acetal homopolymer with UV stabilizers.Aartel 2100UV is a medium viscosity resin with excellent flow characteristics.Aartel 2100UV is available in natural white and may be.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical 80HFICELLHK SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical 95HCTC SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Lighter, Cosmetic Container, ToothbrushCAS No. 9003-54-7Information provided by LG Chemical |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical TR551 MABS, High Transparency, High Rigidity, High Hardness Feature: Injection Molding, High Transparency, High Rigidity, High HardnessApplication: Electric/Electronic Parts Copier, Compact Cases etc.CAS No. 9011-14–7 and 9003-56-9Information provided b.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical TR551 MABS, High Transparency, High Rigidity, High Hardness Feature: Injection Molding, High Transparency, High Rigidity, High HardnessApplication: Electric/Electronic Parts Copier, Compact Cases etc.CAS No. 9011-14–7 and 9003-56-9Information provided b.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness 3.00 mm |
122 °F @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 7500-105 Polyvinyl Chloride, Flexible Notes: 105°C General Purpose; RoHS Compliant Features: High Heat Resistance Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness 1.50 mm |
122 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers VESPEL TP-8311 Polyimide Thermoplastic parts from filled PI (polyimide) for balanced mechanical properties and low wear and friction performance in both dry and lubricated high temperature environmentsInformation provided b.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness 0.750 mm |
122 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers VESPEL TP-8311 Polyimide Thermoplastic parts from filled PI (polyimide) for balanced mechanical properties and low wear and friction performance in both dry and lubricated high temperature environmentsInformation provided b.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness 1.50 mm |
122 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Hytrel® G3548L TPC-ET
(Unverified Data**) Hytrel® G3548L is a low modulus grade with nominal hardness of 35D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injec.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical LI912 ASA Description: Good Weatherability, General PurposeApplication: Mail Box, Sprinkler, Sash Joiner, Toy, Satellite Antenna CoverCAS: 26299-47-8Information provided by LG Chemical |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical LI923 Extrusion ASA Description: Good Weatherability, High RigidityApplication: Communication Instrument Cover, Cable Connecting Cover, Door PanelCAS: 26299-47-8Information provided by LG Chemical |