Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources NY6-GP1 General Purpose Nylon 6 General Purpose Nylon 6, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 5.99 mm |
185 °F @Thickness 0.236 in |
UL 746 |
Polymer Resources NY6-GP1 General Purpose Nylon 6 General Purpose Nylon 6, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 3.00 mm |
185 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources NY6-GP1-[color]-H General Purpose Nylon 6, Heat Stabilized General Purpose Nylon 6, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 3.00 mm |
185 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources NY6-GP2 General Purpose Nylon 6, Nucleated General Purpose Nylon 6, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 5.99 mm |
185 °F @Thickness 0.236 in |
UL 746 |
Polymer Resources NY6-GP2 General Purpose Nylon 6, Nucleated General Purpose Nylon 6, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources NY6-GP2-[color]-H General Purpose Nylon 6, Nucleated, Heat Stabilized General Purpose Nylon 6, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 3.00 mm |
185 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources NY6-GP2-[color]-H General Purpose Nylon 6, Nucleated, Heat Stabilized General Purpose Nylon 6, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 5.99 mm |
185 °F @Thickness 0.236 in |
UL 746 |
Polymer Resources NY6-GP2-[color]-H General Purpose Nylon 6, Nucleated, Heat Stabilized General Purpose Nylon 6, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Delrin® 100AF Acetal Homopolymer
(Unverified Data**) Delrin® 100AF is a high viscosity acetal homopolymer containing 20% Teflon® PTFE fibers. It is designed for applications requiring low wear and/or low friction against steel, itself, and other pla.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 3.00 mm |
185 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Delrin® 100AF Acetal Homopolymer
(Unverified Data**) Delrin® 100AF is a high viscosity acetal homopolymer containing 20% Teflon® PTFE fibers. It is designed for applications requiring low wear and/or low friction against steel, itself, and other pla.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Delrin® 500P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin® 500P has improved processing thermal stability compared to Delrin® 500.Infor.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 0.750 mm |
185 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Delrin® 500T BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 500T BK602 is a toughened, medium viscosity acetal homopolymer resin with impact resistance similar to Delrin® 100. It can be used in parts requiring noise reduction.Information provided b.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Delrin® 500T BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 500T BK602 is a toughened, medium viscosity acetal homopolymer resin with impact resistance similar to Delrin® 100. It can be used in parts requiring noise reduction.Information provided b.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 3.00 mm |
185 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Delrin® 500T BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 500T BK602 is a toughened, medium viscosity acetal homopolymer resin with impact resistance similar to Delrin® 100. It can be used in parts requiring noise reduction.Information provided b.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 3.00 mm |
185 °F @Thickness 0.118 in |
|
Aardvark Polymers Aardalloy® 3300 POM Alloy Rotational Molding Resin Aardalloy 3300 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3300 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® MX 1002 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 3.00 mm |
185 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746B |
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 0.750 mm |
185 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 0.750 mm |
185 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R535 Nylon 66, 35% Glass Reinforced, DAM Vydyne® R535 is general-purpose, hydrolysis-resistant, 35% glass-fiber reinforced PA66 resin. This product is lubricated for improved flow and offers superior surface appearance. Glass-reinforced V.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R535 Nylon 66, 35% Glass Reinforced, DAM Vydyne® R535 is general-purpose, hydrolysis-resistant, 35% glass-fiber reinforced PA66 resin. This product is lubricated for improved flow and offers superior surface appearance. Glass-reinforced V.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R540 Nylon 66, 40% Glass Reinforced, DAM Vydyne® R540 is general-purpose, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 6.00 mm |
185 °F @Thickness 0.236 in |
UL 746B |
DuPont Performance Polymers Delrin® 577 BK000 Acetal Homopolymer
(Unverified Data**) Delrin® 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler, with high stiffness, low warpage and low creep for superior performance at elevated temperature. It con.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 0.750 mm |
185 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R530 NAT Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530 NAT is general-purpose, injection-molding grade, 30% glass-fiber reinforced PA66 resin. Available in natural, it is lubricated for good machine feed, flow and mold releaseAvailability:.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R530 NAT Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530 NAT is general-purpose, injection-molding grade, 30% glass-fiber reinforced PA66 resin. Available in natural, it is lubricated for good machine feed, flow and mold releaseAvailability:.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
|
Aardvark Polymers Aardalloy® 3326 POM Alloy Rotational Molding Resin Aardalloy 3326 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3326 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 3.00 mm |
185 °F @Thickness 0.118 in |
|
Aardvark Polymers Aardalloy® 3326 POM Alloy Rotational Molding Resin Aardalloy 3326 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3326 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 25WSP Nylon 66, Dry as Molded Vydyne® 25WSP is a black, weather-resistant injection-molding grade PA66 resin. This resin offers a well-balanced combination of engineering properties characterized by high strength, rigidity, goo.. |