Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 50.0 °C @Thickness 0.750 mm |
122 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Delrin® 100AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100AL NC010 an unreinforced, high viscosity, lubricated acetal homopolymer resin, containing an advanced system of lubrication for low wear and friction against metals and plastics.Informat.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness 3.00 mm |
122 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Delrin® 100AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100AL NC010 an unreinforced, high viscosity, lubricated acetal homopolymer resin, containing an advanced system of lubrication for low wear and friction against metals and plastics.Informat.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness 0.750 mm |
122 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Delrin® 100P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 100P is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin® 100P provides maximum toughness in the product line without modification. Delrin® 100P has improved pro.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness 0.750 mm |
122 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Delrin® 311DP BK402 Acetal Homopolymer
(Unverified Data**) Delrin® 311DP BK402 is a medium high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Informatio.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness 0.750 mm |
122 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Delrin® 500CL BK601 Acetal Homopolymer
(Unverified Data**) Delrin® 500CL BK601 is a medium viscosity acetal homopolymer containing a chemical lubricant, designed for low wear and friction against metals.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical ALPHALAC SG910 HIPS High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include housing of electric appliancesCA.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical ALPHALAC SG960 HIPS Description: Injection Molding, General Purpose, Good ProcessabilityApplication: Washer Cover, Air-conditioner Panel, Refrigerator PartsCAS No. 9003-55-8Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical ALPHALAC SG970 HIPS Description: Injection Molding, General Purpose, Good Processability, High glossApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical GPPS 15NF(I) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: Food Container, Merchandise, Artificial Woods, Refrigerator Vegetable Box, PSP, Sheet, Film, etc.CAS: 9003-53-6-5In.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical GPPS 20HR(E) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=2.50 mm |
122 °F @Thickness >=0.0984 in |
|
LG Chemical HIPS 405AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 158725-44-1 and 1309-64-4Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical HIPS 410AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical HIPS 501S PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: Refrigerator Food Holder, Food Container, Plastic Toy, Sheet or Film of Yot ReceptacleCAS: 9003-55-8Information provi.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical HIPS 65IHE PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: Refrigerator Tray, Food Tray, Refrigerator Door LinerCAS: 9003-55-8Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=6.00 mm |
122 °F @Thickness >=0.236 in |
|
LG Chemical HIPS 65IHE PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: Refrigerator Tray, Food Tray, Refrigerator Door LinerCAS: 9003-55-8Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical HIPS MI730 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical HIPS MI750L PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical KEYFLEX BT 1072D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical KEYFLEX BT 1172D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=6.00 mm |
122 °F @Thickness >=0.236 in |
|
LG Chemical LI911 ASA Description: Good Weatherability, High FlowApplication: Air-conditioner grill, Sawing Machine Cover, Electric/Electronic ApplicationsCAS: 26299-47-8Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical LUMAX HR5107 PBT+ABS+GF10%, Heat Resistance Description: Injection Molding Grade, PBT+ABS+GF10%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5, 25038-59-9 and 9003-54-7Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness <=3.00 mm |
122 °F @Thickness <=0.118 in |
|
LG Chemical 80HF SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness <=3.00 mm |
122 °F @Thickness <=0.118 in |
|
LG Chemical 82TR SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness <=1.50 mm |
122 °F @Thickness <=0.0591 in |
|
LG Chemical 95HCTC SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Lighter, Cosmetic Container, ToothbrushCAS No. 9003-54-7Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical ALPHALAC SG970NSU HIPS Description: Injection Molding, General Purpose, Good Processability, High gloss, antistatic and UV stabilizedApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical TR551 MABS, High Transparency, High Rigidity, High Hardness Feature: Injection Molding, High Transparency, High Rigidity, High HardnessApplication: Electric/Electronic Parts Copier, Compact Cases etc.CAS No. 9011-14–7 and 9003-56-9Information provided b.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness 1.50 mm |
122 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers VESPEL TP-8311 Polyimide Thermoplastic parts from filled PI (polyimide) for balanced mechanical properties and low wear and friction performance in both dry and lubricated high temperature environmentsInformation provided b.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical HIPS MI750 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical LI912 ASA Description: Good Weatherability, General PurposeApplication: Mail Box, Sprinkler, Sash Joiner, Toy, Satellite Antenna CoverCAS: 26299-47-8Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=6.00 mm |
122 °F @Thickness >=0.236 in |
|
LG Chemical LI923 Extrusion ASA Description: Good Weatherability, High RigidityApplication: Communication Instrument Cover, Cable Connecting Cover, Door PanelCAS: 26299-47-8Information provided by LG Chemical |