Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 0.851 mm |
185 °F @Thickness 0.0335 in |
UL 746 |
Polymer Resources TP-FR-IM-[color]-3 Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 1.60 mm |
185 °F @Thickness 0.0630 in |
UL 746 |
Polymer Resources TP-FR-IM-[color]-3 Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Delrin® 500CL BK601 Acetal Homopolymer
(Unverified Data**) Delrin® 500CL BK601 is a medium viscosity acetal homopolymer containing a chemical lubricant, designed for low wear and friction against metals.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 3.00 mm |
185 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Delrin® 500T BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 500T BK602 is a toughened, medium viscosity acetal homopolymer resin with impact resistance similar to Delrin® 100. It can be used in parts requiring noise reduction.Information provided b.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 0.710 mm |
185 °F @Thickness 0.0280 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 101F BKB009 Nylon 66
(Unverified Data**) Zytel® 101F BKB009 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 0.750 mm |
185 °F @Thickness 0.0295 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 8018HS BKB085 Nylon 66
(Unverified Data**) Zytel® 8018HS BKB085 is a 14% glass reinforced, toughened, heat stabilized black polyamide 66 resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness >=3.00 mm |
185 °F @Thickness >=0.118 in |
|
LG Chemical AF305HT ABS, Flame Retardant, Heat Resistance Feature: Injection Molding, Flame Retardant, Heat ResistanceApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 9001-96-2, 68928-70-1, and 1309-64-4Inf.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness >=2.50 mm |
185 °F @Thickness >=0.0984 in |
|
LG Chemical LUPOY GN5001RFJ PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (OA Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 0.750 mm |
185 °F @Thickness 0.0295 in |
|
Eurostar Starflam P10002E PA6, Injection Molded Starflam P10002E is a Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding Resin (also known as P1000Z220 or PA6 U2 Z22)Information provided by Polymer Tec.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
|
Eurostar Starflam P10002E PA6, Injection Molded Starflam P10002E is a Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding Resin (also known as P1000Z220 or PA6 U2 Z22)Information provided by Polymer Tec.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 0.800 mm |
185 °F @Thickness 0.0315 in |
|
Eurostar Starflam R10002E PA66/6, Injection Molded Starflam R10002E is a Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 66/Polyamide 6 Injection Molding Resin (also known as R1000Z220EM)Information provided by Polymer Te.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 0.710 mm |
185 °F @Thickness 0.0280 in |
UL 746 |
Ascend Performance Materials Vydyne® 20NSP Nylon 66, DAM Vydyne® 20NSP is a general-purpose, highly nucleated, lubricated PA66 resin available in natural color. It is designed to crystallize rapidly in order to reduce cycle times and increase productivit.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 3.00 mm |
185 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 43% Filler by Weight Additive:Nucleating AgentLubricant Features:Fast Molding CycleGeneral PurposeGood Mold Release Good.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 0.710 mm |
185 °F @Thickness 0.0280 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPC Nylon 66, DAM Vydyne® 21SPC is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding fabrication. This resin offers a well balanced combination of engineering .. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPC1 Nylon 66, DAM Vydyne® 21SPC1 is a general-purpose, improved-flow, lubricated PA66 resin available in natural color. 21SPC1 offers a balanced combination of properties characterized by high strength, rigidity, go.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 0.710 mm |
185 °F @Thickness 0.0280 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, Conditioned Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 3.00 mm |
185 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, Conditioned Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 3.00 mm |
185 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose, High Productivity, DAM Vydyne® 21SPF is general-purpose PA66 resin. Available in natural, it is designed principally for injection-molding fabrication. This grade offers a well-balanced combination of engineering propert.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 3.00 mm |
185 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 49 Nylon 66, DAM Vydyne® 49 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 3.00 mm |
185 °F @Thickness 0.118 in |
UL 746B |
Ascend Performance Materials Vydyne® 66B, 66J Nylon 66, Dry as Molded Vydyne® 66B and 66J are members of a family of unreinforced extrusion grade Nylon 66 resins. They are available in natural color. These resins offer high strength, rigidity, and toughness for a bro.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 3.00 mm |
185 °F @Thickness 0.118 in |
UL 746B |
Ascend Performance Materials Vydyne® 50BW Nylon 66, Dry as Molded Vydyne® 50BW is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a high-viscosity resin. This resin offers a well-balanced comb.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 0.810 mm |
185 °F @Thickness 0.0319 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**) Zytel® ST801 is an unreinforced, super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity range and high productivit.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 20NSP BLK Nylon 66, DAM Vydyne® 20NSP BLK is a general-purpose, high nucleated, lubricated PA66 resin. Available in black, it is designed to crystallize rapidly in order to reduce cycle times and increase productivity thr.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, DAM Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 3.00 mm |
185 °F @Thickness 0.118 in |
|
Aardvark Polymers Aardalloy® 3326 POM Alloy Rotational Molding Resin Aardalloy 3326 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3326 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 0.710 mm |
185 °F @Thickness 0.0280 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® EFE1068 NC010T Nylon 66
(Unverified Data**) Zytel® EFE1068 NC010T is a lubricated polyamide 66 for injection molding. It has excellent flow characteristics and was developed for fast production cycles and high productivity applications.Info.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 6.00 mm |
185 °F @Thickness 0.236 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® EFE1068 NC010T Nylon 66
(Unverified Data**) Zytel® EFE1068 NC010T is a lubricated polyamide 66 for injection molding. It has excellent flow characteristics and was developed for fast production cycles and high productivity applications.Info.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® EFE1068 NC010T Nylon 66
(Unverified Data**) Zytel® EFE1068 NC010T is a lubricated polyamide 66 for injection molding. It has excellent flow characteristics and was developed for fast production cycles and high productivity applications.Info.. |
|||
UL RTI, Mechanical without Impact | 85.0 °C @Thickness 3.00 mm |
185 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, DAM Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding .. |