Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable WEJB400LU Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D746 |
PolyOne Geon™ HC 2180 Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2180 is a 80 Shore A non-phthalate flexible vinyl compound made from FDA sanctioned ingredients. HC 2180 can be used for extrusion and injection molding healthcare applications.NOTE: All ing.. |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible MG26 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible XV3856 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | F<sub>50</sub>, Test method has been found useful for specification purposes, but does not necessarily indicate the lowest temperature at which the material may be used.; ASTM D746 |
LyondellBasell Petrothene® NA870252 Low Density Polyethylene ApplicationsPETROTHENE NA 870-252 exhibits an excellent balance of toughness and softness, with excellent dimensional stability. Typical applications include caps and closures, housewares, toys, co.. |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | |
Spartech 2850-80 PVC for Regulated Applications Information provided by Spartech |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D746 |
Teknor Apex APEX® 3611-90 Polyvinyl Chloride, Flexible Uses: Medical/Healthcare Applications Agency Ratings: NSF 61 Forms: Pellets Additional Information: Second Generation SeriesInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D746 |
Teknor Apex APEX® 84855 Polyvinyl Chloride, Flexible Notes: 105°C Jacket; RoHS Compliant Features: Flame Retardant; Sunlight Resistant (720 hours) Uses: Cable Jacketing Forms: Pellets Agency Ratings: UL QMTT2 .E73402; UL 62 Wire Types: SJTW; STWInf.. |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D746 |
Teknor Apex APEX® 89-P129A-NT Polyvinyl Chloride, Flexible Notes: RoHS Compliant Features: High Heat Resistant; Low to no Migration; Oil Resistant Uses: Flexible Cord Jacketing Agency Ratings: UL 62 Forms: PelletsInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D746 |
Teknor Apex Fireguard® 910L16-C1A-NL1 Polyvinyl Chloride, Flexible Notes: RoHS Compliant Features: Flame Retardant; Low Smoke Emission Uses: Plenum Cable Jacketing Wire Types: CL2P; CL3P; CMP; FPLP; MPP; OFNP Agency Ratings: NEC Article 725; NEC Article 760; NEC Ar.. |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D746 |
Teknor Apex APEX® 01-A0383A-85 Polyvinyl Chloride, Flexible Notes: 105°C Insulation; RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D746 |
Teknor Apex APEX® 94-A0098A-84 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-Natural Color, OpaqueForms-PelletsProcessing Method-I.. |
|||
Brittleness Temperature | <= -25.0 °C | <= -13.0 °F | passes at 3 min.; ASTM D2137 |
Vicone High Performance Rubber VicoFluor™ 57FK-GR High Performance Fluoroelastomer Rubber Meets ASTM D2000 fluoroelastomer 75 Durometer. |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GS 7802 Flexible PVC, Injection Molding for Footwear Soles |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GSO 65/33 Flexible PVC, Injection Molding for Footwear Soles, opaque surface |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | |
Colorite Polymers Self Frosting™ 8511SF Vinyl Compound Description: Colorite has developed a family of vinyl compounds to satisfy the needs of those who need a smooth, low gloss, low friction surface for the products that they produce. Historically, thi.. |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | |
Colorite Polymers 8511 Clear Extrusion Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre.. |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | |
Colorite Polymers 8512 Clear Injection Molding Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c.. |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PHT 0144 Flexible PVC, Transparent Extrusion Profiles high temperatures |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D-746 |
Axiall 21540 Coax & Telecom Flexible PVC Semi-rigid flame retardant insulation compound with good electrical properties for minimum transmission interference. Suitable for use in riser insulation.Information provided by Georgia GulfGeorgi.. |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D-746 |
Axiall 38951 Wire & Cable Flexible PVC Low cost AWM jacket for SPT, SVT, SJT applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | |
AlphaGary GW 3042 LCF Flame Retardant Polyvinyl Chloride 75°C rated jacket compound |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D-746 |
Axiall 19854 Wire & Cable Flexible PVC Non-lead stabilized, 105°C rated insulation compound. Recognized by UL for TW and THW applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D746 |
Teknor Apex APEX® 3311-85 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | |
AlphaGary PVC GM 5075 Polyvinyl Chloride Thermoplastic A 105°C rated, lead & cadmium free, UL-94 V2 molding compound |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GS 80/T Flexible PVC, Injection Molding for Footwear Soles and sandals |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PM 6805 Flexible PVC, Lead Free Various profiles |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PM 8005 Flexible PVC, Lead Free Various profiles |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | ASTM D-746 |
Axiall 8424 Moldings & Extrusions Flexible PVC A clear, outdoor grade extrusion compound formulated for good UV light resistance and good low temperature properties. Recommended for fence coating applications.Information provided by Georgia Gul.. |
|||
Brittleness Temperature | -25.0 °C | -13.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PM 8030 Flexible PVC, Lead Free Furniture border |