Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable EHA70L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable W2403 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable WJJC330 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746-98 |
Rogers Corporation Poron® 4790-92-12 Urethane Foam, Extra Soft, Slow Rebound Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746-98 |
Rogers Corporation Poron® 4790-92-15 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Extra soft, slow rebound with a very low closure force.Features and Benefits of PORON Products: Excellent compression set resistance which enables durable, long-term performance for gasketing, seali.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746-98 |
Rogers Corporation Poron® 4790-92-15 Urethane Foam, Extra Soft, Slow Rebound Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
Brittleness Temperature | <= -20.0 °C | <= -4.00 °F | ASTM D746 |
Polimeri Europa Riblene® MR 10 R Low Density Polyethylene - Injection Molding Riblene MR 10 R is a high fluidity low density polyethylene resin (LDPE).Parts made with Riblene MR 10 R are characterized by a high flexibility.Main Applications: Riblene MR 10 R is suitable for i.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible A4DU5 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible B5DU0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
S&E Specialty Polymers TufTech™ GA-8705-03 Natural PVC Compound Application: A 75°C, RoHS compliant, PVC based compound, suitable for Riser jacketing applications.Information provided by S&E Specialty Polymers |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible P484B Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R5230C Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | <= -20.0 °C | <= -4.00 °F | ASTM D 746 |
Karina 65/200 Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
Teknor Apex Fireguard® 910L16-C6-NL1 Polyvinyl Chloride, Flexible Notes: RoHS Compliant Features: Flame Retardant; Low Smoke Emission Uses: Plenum Cable Jacketing Wire Types: CL2P; CL3P; CMP; FPLP; MPP; OFNP Agency Ratings: NEC Article 725; NEC Article 760; NEC Ar.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
Teknor Apex APEX® 01-A0303E-95 Polyvinyl Chloride, Flexible Notes: 105°C Insulation; RoHS Compliant Uses: Automotive Electronics; Insulation; Wire and Cable Applications Wire Types: GPT Agency Ratings: SAE J1128 Forms: PelletsInformation Provided by Tekno.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
Teknor Apex APEX® 3801-90 Polyvinyl Chloride, Flexible Features: Non-DEHP Plasticizer; Ethylene Oxide Sterilizable; High Heat Resistance Uses: Medical/Healthcare Applications Processing Method: Extrusion Forms: PelletsInformation Provided by Teknor Apex.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
SCG Chemicals EL-Proâ„¢ P740J Polypropylene Injection Molding Key Characteristics:Good flowabilityGood processabilityHigh stiffnessRecommended Applications:Automotive, motorcycle and electrical appliance parts that require good flowability such as automotive t.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
SCG Chemicals EL-Proâ„¢ P841J Polypropylene Injection Molding Key Characteristics:Excellent flowabilityExcellent processabilityHigh stiffnessSuitable for complex parts and large partsContains UV stabilizer and anti-static agentRecommended Applications:Electric.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
SCG Chemicals EL-Proâ„¢ P852J Polypropylene Injection Molding Key Characteristics:Excellent productivityHigh clarityHigh stiffnessRecommended Applications:Clear food containerClear large size containerHousehold products and other articles that require high tra.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | Molded and tested in accordance with ASTM D4976; ASTM D746 |
Dow DNDA-1082 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-1082 NT 7 is produced using UNIPOL™ PE process technology. It is intended for high-speed injection molding of thin walled parts such as downguaged lids. Information provided by Dow |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
Colorite Polymers CS8042SC Wire and Cable Jacket Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PG 86/AF Flexible PVC, Extrusion Modified with Rubber Profiels UL 94 Classe V0 |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D-746 |
Axiall 384FR Wire & Cable Flexible PVC Highly flame retardant jacketing compound recommended for direct burial applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D-746 |
Axiall 830 Wire & Cable Flexible PVC TW insulation. UL recognized for TW and Oil resistant II.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D-746 |
Axiall 8916 Moldings & Extrusions Flexible PVC A satin finish extrusion compound best suited for extruded T-moldings, tubings and other shapes where uniform flow through the die is required. The compound exhibits excellent abrasion resistance.I.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D-746 |
Axiall 8940 Moldings & Extrusions Flexible PVC General purpose semi-rigid extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | |
Aearo E-A-R Specialty Composites Isodamp® C-1000 Series TPE Isodamp® C-1000 Series TPEs feature high internal damping properties for low amplification at resonance to protect equipment during frequency cycling and random shocks, effective shock protection f.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable W1201 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | |
AlphaGary PVC GM 8001-E Natural LCF Polyvinyl Chloride Thermoplastic A lead free, flame retarded, V-O rated compound designed for plug molding |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
SCG Chemicals EL-Pro™ P441JU Polypropylene Injection Molding Key Characteristics:Excellent impact strengthContains UV stabilizer and anti-static agentSuitable for small to medium partsRecommended Applications:High impact and durable automotive and electrical .. |