Polymer Property : Brittleness Temperature = -29.2 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature -34.0 °C
-29.2 °F
ASTM D746
PolyOne Geon™ Vinyl Wire & Cable 2510-xx05D Polyvinyl Chloride Alloy (PVC Alloy)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Brittleness Temperature -34.0 °C
-29.2 °F
ASTM D746
S&E Specialty Polymers GA-509ORLT PVC
Application: Lead free, flame retardant UV and oil resistant PVC jacketing compound with superior low temperature properties.Information provided by S&E Specialty Polymers
Brittleness Temperature -34.0 °C
-29.2 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible 90451 Polyvinyl Chloride, Flexible (PVC, Flexible)
Automotive OEM approval(s).Information provided by PolyOne
Brittleness Temperature -34.0 °C
-29.2 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible WR3090S Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Brittleness Temperature -34.0 °C
-29.2 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible R3090S Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Brittleness Temperature -34.0 - -17.0 °C
-29.2 - 1.40 °F
Average value: -22.7 °C Grade Count:7
Overview of materials for Polybutene
This property data is a summary of similar materials in the MatWeb database for the category "Polybutene". Each property range of values reported is minimum and maximum values of appropriate MatWeb ..
Brittleness Temperature -34.0 °C
-29.2 °F
ASTM D746
LyondellBasell DP 8310M Polybutene
Key Features: semi-crystalline high ethylene content random copolymerApplications: packaging industry, cast film, FDA acceptableMeets FDA requirements in 21 CFR 177.1570 for direct food contact up t..
Brittleness Temperature -34.0 °C
-29.2 °F
ASTM D746
LyondellBasell DP 8510M Polybutene
Key Features: semi-crystalline high ethylene content random copolymer, miscible with polyproylenesApplications: Hot Melt Adhesives, FDA acceptableMeets FDA requirements in 21 CFR 175.105 for indirec..
Brittleness Temperature -34.0 °C
-29.2 °F
Sylvin Technologies 6161-82 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
Brittleness Temperature -34.0 °C
-29.2 °F
ASTM D746
Teknor Apex APEX® 157V-4 LG Polyvinyl Chloride, Flexible
Notes: RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex
Brittleness Temperature -34.0 °C
-29.2 °F
ASTM D746
Teknor Apex APEX® 3601-80 Polyvinyl Chloride, Flexible
Uses: Medical/Healthcare Applications Agency Ratings: NSF 61 Forms: Pellets Additional Information: Second Generation SeriesInformation Provided by Teknor Apex
Brittleness Temperature -34.0 °C
-29.2 °F
ASTM D746
Teknor Apex APEX® 3700-80 Polyvinyl Chloride, Flexible
Features: DEHP Plasticizer; Ethylene Oxide Sterilizable; High Heat Resistance Uses: Medical/Healthcare Applications Processing Method: Extrusion Forms: PelletsInformation Provided by Teknor Apex
Brittleness Temperature -34.0 °C
-29.2 °F
ASTM D746
Teknor Apex APEX® 3800-80 Polyvinyl Chloride, Flexible
Features: DEHP Plasticizer; Ethylene Oxide Sterilizable; High Heat Resistance Uses: Medical/Healthcare Applications Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor ..
Brittleness Temperature -34.0 °C
-29.2 °F
ASTM D746
Teknor Apex APEX® 85-J644-H Polyvinyl Chloride, Flexible
Notes: 105°C Jacket; RoHS Compliant Features: Flame Retardant; High Heat Resistance; Low gloss Uses: Communication Wire Jacketing; Patch Cord Jacketing Forms: Pellets Agency Ratings: NEC Article ..
Brittleness Temperature -34.0 °C
-29.2 °F
ASTM D746
Teknor Apex APEX® 94-A1235-C-75-NT1 Polyvinyl Chloride, Flexible
Notes: RoHS Compliant Forms: PelletsInformation Provided by Teknor Apex
Brittleness Temperature -34.0 °C
-29.2 °F
ASTM D746
Teknor Apex MF 181 NT Polyvinyl Chloride, Flexible Film
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Film, Medical Applications Forms-PelletsAppearance-ClearAgency Ratings- FDA Unspecified RatingInformatio..
Brittleness Temperature -34.0 °C
-29.2 °F
Cold Flex; ISO 458/2
Fainplast Compounds GK 85/UV Flexible PVC, Flame Retardant Sheathing Lead Free
Sheathing low temperatures
Brittleness Temperature -34.0 °C
-29.2 °F
Fainplast Compounds GS 87/BT Flexible PVC, Injection Molding for Transparent Technical Items
Technical items low temperatures
Brittleness Temperature -34.0 °C
-29.2 °F
Cold Flex; ISO 458/2
Fainplast Compounds PH 65/A Flexible PVC, Transparent Extrusion
Transparent profiles
Brittleness Temperature -34.0 °C
-29.2 °F
Cold Flex; ISO 458/2
Fainplast Compounds PH 66/A Flexible PVC, Transparent Extrusion
Profiles, UL Class V2
Brittleness Temperature -34.0 °C
-29.2 °F
ASTM D-746
Axiall 39012 Coax & Telecom Flexible PVC
Flame retardant CATV and general purpose jacket. UL recognized for sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Brittleness Temperature -34.0 °C
-29.2 °F
ASTM D746
Teknor Apex APEX® 7500-85 Polyvinyl Chloride, Flexible
Notes: 105°C General Purpose; RoHS Compliant Features: High Heat Resistance Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL Q..
Brittleness Temperature -34.0 °C
-29.2 °F
Cold Flex; ISO 458/2
Fainplast Compounds PM 64/OP Flexible PVC, Lead Free
Gaskets, Opaque surface
Brittleness Temperature -34.0 °C
-29.2 °F
ASTM D746-79
DuPont Performance Polymers Hypalon® 40 Chlorosulfonated Polyethylene Rubber, Mineral Filled Compound  (discon
Mineral filled compound with 100 parts Hypalon; 80 parts hard clay; 4 parts magnesia; 30 parts aromatic process oil; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont ..
Brittleness Temperature -34.0 °C
-29.2 °F
ASTM D746-79
DuPont Performance Polymers Hypalon® 4085 Chlorosulfonated Polyethylene Rubber, Mineral Filled Compound  (disc
Mineral filled compound with 100 parts Hypalon; 80 parts hard clay; 4 parts magnesia; 30 parts aromatic process oil; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont ..