Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable 1802-xx17FRD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable EMB405L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable W3200 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable WJJC34L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible A4D00 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R999A Black Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible XV3784 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable WJJC310L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R5230C Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
Teknor Apex APEX® 2090-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-ClearForms-PelletsProcessing Method-Extrusi.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
Teknor Apex APEX® 3200-90 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
Teknor Apex APEX® 94-A0098C-85 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-ClearForms-PelletsProcessing Method-Injection Molding.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
Teknor Apex APEX® 3801-90 Polyvinyl Chloride, Flexible Features: Non-DEHP Plasticizer; Ethylene Oxide Sterilizable; High Heat Resistance Uses: Medical/Healthcare Applications Processing Method: Extrusion Forms: PelletsInformation Provided by Teknor Apex.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
Teknor Apex MF 170 NT Polyvinyl Chloride, Flexible Film Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Film, Medical Applications Forms-PelletsAppearance-ClearInformation provided by Teknor Apex Company |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
SCG Chemicals EL-Proâ„¢ P722JO Polypropylene Injection Molding Key Characteristics:Good flowabilityGood sealabilityGood mechanical property balanceMinimal shrinkage and warpageContains UV stabilizerRecommended Applications:Good impact automotive and electrical .. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
SCG Chemicals EL-Proâ„¢ P740J Polypropylene Injection Molding Key Characteristics:Good flowabilityGood processabilityHigh stiffnessRecommended Applications:Automotive, motorcycle and electrical appliance parts that require good flowability such as automotive t.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
SCG Chemicals EL-Proâ„¢ P842J Polypropylene Injection Molding Key Characteristics:Excellent flowabilityExcellent processabilityExcellent stiffnessSuitable for complex parts and large partsRecommended Applications:Electrical appliance parts, mainly for refriger.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | Molded and tested in accordance with ASTM D4976; ASTM D746 |
Dow DMDA-8965 NT 7 High Density Polyethylene Resin DOW DMDA-8965 NT 7 is produced using UNIPOL™ process technology. It is intended for use in thin wall injection molding applications such as food containers. Information provided by Dow |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GSO 70/33 Flexible PVC, Injection Molding for Footwear Soles, opaque surface |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PMS 75 Flexible PVC, Lead Free Gas pipes stabilized Ca-Zn |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
Colorite Polymers CS1539GP Wire and Cable Insulation Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
Colorite Polymers CS6037GP Wire and Cable Insulation Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | |
Colorite Polymers 9012 Clear Injection Molding Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PG 86/AF Flexible PVC, Extrusion Modified with Rubber Profiels UL 94 Classe V0 |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D-746 |
Axiall 1131-57D Wire & Cable Flexible PVC Non-lead stabilized 105°C rated jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D-746 |
Axiall 19940 Wire & Cable Flexible PVC 105°C rated insulation compound for 600V, 1/64 wall (18 AWG and larger) and 1000V applications. Approved by UL for THWN-2 (8 AWG and larger) and THW-2 in all sizes and colors. UL approved for 94 .. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D-746 |
Axiall 34551 Wire & Cable Flexible PVC TW, THW insulation also suitable for 105°C AWM, flex cords and Class 12/12B insulations.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | ASTM D746 |
Colorite Polymers 5376FFR General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | |
AlphaGary PVC GM 8001-E Natural LCF Polyvinyl Chloride Thermoplastic A lead free, flame retarded, V-O rated compound designed for plug molding |
|||
Brittleness Temperature | -20.0 °C | -4.00 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PM 8220 Flexible PVC, Lead Free Various profiles |