Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable W1100L-xx93FRSD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
PolyOne OnFlex™ HFFR 310-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 310-01 is a non-halogen flame retardant material designed for cable jackets. New Product. Commercial specifications have not been established. - Non-halogen flame retardant - UL62 comp.. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
Advanced Elastomer Systems VistaFlex® 912-B Thermoplastic Rubber
(discontinued **) Description: A black super high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as .. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
PolyOne Geon™ HC 2155 Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2155 is a 55 Shore A non-phthalate flexible vinyl compound made from FDA sanctioned ingredients. HC 2155 can be used for extrusion and injection molding healthcare applications.NOTE: All ing.. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible 86479 Tran Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D 746 |
Karina 809D48/1-C-IS-LMP Black PVC Compound Heavy metal free PVC compound recommended for extrusion of coaxial cables jacket. Also recommended for extrusion of automotive flexible tube. Working temperature range: -40°C to +80°C.Inform.. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D746 |
SABIC Innovative Plastics NORYL WCA105 PPE-TPE (Europe-Africa-Middle East) Flexible, non-halogenated FR mPPE extrusion grade ideal for evaluation in applications such as wire insulation. Flame retardant performance capable of meeting VW1 and 105C temperature rating requir.. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D746 |
SABIC Innovative Plastics NORYL WCD771 PPE-TPE (Asia Pacific) Flexible, high tensile elongation, halogen-free extrusion grade intended for evaluation in applications such as cable jacket. Flame retardant performance capable of meeting UL VW-1 requirement. 80C .. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D746 |
SABIC Innovative Plastics NORYL WCD825 PPE-TPE (Asia Pacific) Flexible, very low-migration, halogen-free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame retardant performance capable of meeting UL VW-1 re.. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D746 |
SABIC Innovative Plastics NORYL WCD835 PPE-TPE Flexible, low odor, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements. 80C end.. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D746 |
SABIC Innovative Plastics NORYL WCD855 PPE-TPE (Asia Pacific) Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as cable jacket of UL 62 SPE and NISPE confiations. Flame retardant performance capable of m.. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D746 |
SABIC Innovative Plastics NORYL WCD861A PPE-TPE (Asia Pacific) Flexible, migration-improved, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements.. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D746 |
SABIC Innovative Plastics NORYL WCD933 PPE-TPE Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as insulation of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN.. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D746 |
SABIC Innovative Plastics NORYL WCP821 PPE-TPE (Asia Pacific) Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain .. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D746 |
SABIC Innovative Plastics NORYL WCP821 PPE-TPE (Europe-Africa-Middle East) Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain .. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
Seals Eastern 7182X Fluorocarbon-Elastomer Formulated AFLAS®. Ultra-low compressive stress relaxation for alkaline, high-temperature service.Information provided by Seals Eastern, Inc. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | |
Sibur O-40 Compound OM-40 Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
Teknor Apex APEX® 3070-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin.. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
Teknor Apex APEX® 3700-70NT1 Polyvinyl Chloride, Flexible Features: DEHP Plasticizer; Ethylene Oxide Sterilizable; High Heat Resistance Uses: Medical/Healthcare Applications Processing Method: Extrusion Forms: PelletsInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
Teknor Apex Flexalloy® 3501-75-NT Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppe.. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D746 |
SABIC Innovative Plastics NORYL WCD841U PPE-TPE Flexible, UV stabilized, halogen free extrusion grade for applications such as wire insulation and cable jacket. Good color stability after UV weathering per ASTM D4459. Light color capable. Flame r.. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D746 |
SABIC Innovative Plastics NORYL WCD883 PPE-TPE (Europe-Africa-Middle East) Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as jacket of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN 502.. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D746 |
SABIC Innovative Plastics NORYL WCD933 PPE-TPE (Europe-Africa-Middle East) Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as insulation of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN.. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GS 55 Flexible PVC, Injection Molding for Footwear Tennis shoes |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PG 55/A Flexible PVC, Extrusion Modified with Rubber Gaskets modified with rubber |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D2137 |
Aearo E-A-R Specialty Composites VersaDamp™ V-2325 TPE VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded.. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D-746 |
Axiall 8752 Moldings & Extrusions Flexible PVC Low gravity, flame retardant extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
Alliance Polymers Zythane™ 7080A Thermoplastic Polyurethane Elastomer Zythane™ 7080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Brittleness Temperature | -40.0 °C | -40.0 °F | ASTM D746 |
Colorite Polymers 7075 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Brittleness Temperature | <= -40.0 °C | <= -40.0 °F | ASTM D746 |
SABIC Innovative Plastics NORYL WCD835 PPE-TPE (Asia Pacific) Flexible, low odor, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements. 80C end.. |