Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
Polimeri Europa Eraclene® MM 84 High Density Polyethylene - Injection Molding Eraclene MM 84 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MM 84 is characterized by high rigidity and good impact resistance. .. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible XV3845 Polyvinyl Chloride, Flexible (PVC, Flexible) NOTE: All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | TPE-0089 (ASTM D 746) |
Advanced Elastomer Systems Santoprene® 181-55 Thermoplastic Rubber
(discontinued **) A black thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be proc.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
Polimeri Europa Eraclene® MS 80 High Density Polyethylene - Injection Molding Eraclene MS 80 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MS 80 shows a good balance between processability and mechanical pro.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D746 |
Eastman E6838-850P Polyethylene
(discontinued **) E6838-850P is a low density resin designed for applications where high coating speeds and good drawdown are required. The combination of high melt index and low density also provides good heat seal.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D740 |
LG Chemical LUTENE MB9500 LDPE Injection Molding Grade Description: The physical and structural characteristics of LUTENE MB9500 give it excellent flow properties and good productivity, clarity and surface gloss.Main Application: Powder coating, artific.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | |
Momentive Performance Materials RTV157 High Strength Silicone Adhesive Sealant, Gray RTV 157 is a one component, ready-to-use, high strength silicone rubber adhesive sealant. It cures to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature. RTV15.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | |
Momentive Performance Materials RTV1673LV One Component, Low Volatile Silicone Adhesive Sealant, Black RTV1673LV one-component, ready-to-use adhesive sealants cures to a tough durable, resilient silicone rubber when exposed to atmospheric moisture at room temperature. Methyl alcohol and a small amoun.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | |
Momentive Performance Materials RTV5818 One-Component, Modified Alkoxy Adhesive Sealant, Translucent RTV5810 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature... |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | |
Teknor Apex Elexar® EL 3954-62 Thermoplastic Elastomer Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
SCG Chemicals EL-Leneâ„¢ F15 High Density Polyethylene Film Key Characteristics:High productivityHigh tensile strengthHigh dart impactHigh stiffnessLow gel contentGood moisture barrierExcellent printabilityRecommended Applications:High speed processingWide l.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
SCG Chemicals EL-Leneâ„¢ H1000P High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stabilityRecommended Applications: Water pipes, conduit, sewage drainage pipesInformation provided by SCG Chemicals |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
Teknor Apex TEKRON® 4300-D88A Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
Teknor Apex Telcar® TL-1025-65 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D746 |
Teknor Apex Telcar® TL-1934G Styrenic Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Cable Jacketing; Flexible Cord Insulation; Connectors; Wire Jacketing; Wire and Cable Applications Agency Ratings: UL 1581Forms: Pellets Proces.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
Teknor Apex Telcar® TL-8421 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
Teknor Apex Telcar® TL-8712R Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
Teknor Apex UNIPRENE® 7010-45 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | ASTM D746 |
Teknor Apex Uniprene® UN-2028A UMB Thermoplastic Elastomer Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | JIS K6301 |
Toyobo Pelprene™ S-6001 Polyester TPE Key Feature: Pelprene S typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'S' type is a block.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D 746 |
Zylog Neoplast® 155 FT SWB Thermoplastic Vulcanizate Neoplast 155 FT SWB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.RoHS Compliant,.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D746 |
Teknor Apex Uniprene® UN-7010-55NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D746 |
ExxonMobil Santoprene® 171-64 Thermoplastic Elastomer A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D746 |
Alliance Polymers Viprene™ G45D-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G45D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D746 |
Alliance Polymers Viprene™ G90A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G90A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D746 |
Alliance Polymers Viprene™ P75A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P75A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D 746 |
AlphaGary Evoprene™ LF 6153 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
Brittleness Temperature | -60.0 °C | -76.0 °F | ASTM D746 |
Alliance Polymers Viprene™ G40D-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G40D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | TPE-0089 (ASTM D 746) |
Advanced Elastomer Systems Santoprene® 101-64 W175 Thermoplastic Rubber
(discontinued **) A black thermoplastic general purpose elastomer designed for thin wall extrusion with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfo.. |
|||
Brittleness Temperature | <= -60.0 °C | <= -76.0 °F | TPE-0089 (ASTM D 746) |
Advanced Elastomer Systems Santoprene® 281-45 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |