Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Brittleness Temperature = 82.2 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature <= 82.2 °C
<= 180 °F
ASTM D746
I. Stern IS-35955 High Density Polyethylene, Blow Molding Grade
Features:IS-35955 is designed for applications requiring excellent stiffness and stress crack resistance properties.Meets all requirements of the U. S. Food and Drug Administration as specified in 2..
Copyright © lookpolymers.com All Rights Reserved