Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 875 °C @Thickness 3.20 mm |
1610 °F @Thickness 0.126 in |
Glow Wire Ignition Temperature; IEC 695-2-13 |
Nilit Nilamid A G5 FR C4 25% Glass Fiber Reinforced, Flame Retardant PA66 (with Halogens) Description: Nilamid A G5 FR C4 combines excellent mechanical performance with flame retardancy. The halogenated flame retardant system used in this product allows a wide range of colors. This produ.. |
|||
Glow Wire Test | 875 °C @Thickness 1.00 mm |
1610 °F @Thickness 0.0394 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® FXD9810 PC Copolymer (Europe-Africa-Middle East) Non-chlorinated, non-brominated Flame retardant PC-siloxane copolymer blend. Excellent processability, super high flow, good impact, UL rated V-0. Limited translucent colors.This data was supplied b.. |
|||
Glow Wire Test | 875 °C @Thickness 0.800 mm |
1610 °F @Thickness 0.0315 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Solvay Specialty Polymers Udel® P-1700 Polysulfone (PSU)
(Unverified Data**) Udel P-1700 polysulfone (PSU) is a tough, rigid, high-strength thermoplastics suitable for continuous use up to 300°F (149°C). It is resistant to oxidation and hydrolysis and withstand prolonged e.. |
|||
Glow Wire Test | 875 °C @Thickness 3.00 mm |
1610 °F @Thickness 0.118 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® 19 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 875 °C @Thickness 3.00 mm |
1610 °F @Thickness 0.118 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® 22 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 875 °C @Thickness 3.00 mm |
1610 °F @Thickness 0.118 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® 24 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 875 °C @Thickness 3.00 mm |
1610 °F @Thickness 0.118 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® 24 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 875 °C @Thickness 3.00 mm |
1610 °F @Thickness 0.118 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® G4F 22 R Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 875 °C @Thickness 3.00 mm |
1610 °F @Thickness 0.118 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® G4F 25 UR Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 875 °C @Thickness 3.00 mm |
1610 °F @Thickness 0.118 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® G6F 23 UR Polycarbonate-30% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 875 °C @Thickness 1.00 mm |
1610 °F @Thickness 0.0394 in |
GWIT |
LATI Larpeek 10 G/30 PEEK, 30% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Glow Wire Test | 875 °C @Thickness 3.00 mm |
1610 °F @Thickness 0.118 in |
IEC 60695-2-12 |
Styron CALIBREâ„¢ 301-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300-10 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet appli.. |
|||
Glow Wire Test | 875 °C @Thickness 2.00 mm |
1610 °F @Thickness 0.0787 in |
IEC 60695-2-12 |
Styron CALIBREâ„¢ 301-15 Polycarbonate Resin Overview: CALIBREâ„¢ 300-115 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity. The CALIBREâ„¢ 300-10 series products are available in 4 .. |
|||
Glow Wire Test | 875 °C @Thickness 2.00 mm |
1610 °F @Thickness 0.0787 in |
IEC 60695-2-12 |
Styron CALIBREâ„¢ 303-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300-10 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet appli.. |
|||
Glow Wire Test | 875 °C @Thickness 1.50 mm |
1610 °F @Thickness 0.0591 in |
Glow Wire Ignition Temperature, dry; IEC 60695-2-13 |
DSM Akulon® F-X9183 PA6 Low/Medium Viscosity |
|||
Glow Wire Test | 875 °C @Thickness 3.00 mm |
1610 °F @Thickness 0.118 in |
GWIT; IEC 60695-2-13 |
Covestro Makrolon® 2400 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Glow Wire Test | 875 °C @Thickness 2.00 mm |
1610 °F @Thickness 0.0787 in |
GWIT; IEC 60695-2-13 |
Covestro Makrolon® 2667 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med.. |
|||
Glow Wire Test | 875 °C @Thickness 1.00 mm |
1610 °F @Thickness 0.0394 in |
GWIT; IEC 60695-2-13 |
Covestro Makrolon® 2800 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Glow Wire Test | 875 °C @Thickness 1.00 mm |
1610 °F @Thickness 0.0394 in |
GWIT; IEC 60695-2-13 |
Covestro Makrolon® 3100 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
Glow Wire Test | 875 °C @Thickness 1.50 mm |
1610 °F @Thickness 0.0591 in |
GWIT; IEC 60695-2-13 |
Covestro Makrolon® 3107 MAS167 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
Glow Wire Test | 875 °C @Thickness 0.750 mm |
1610 °F @Thickness 0.0295 in |
GWFI; IEC 60695-2-12 |
Covestro Makrolon® ET3117 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc.. |
|||
Glow Wire Test | 875 °C @Thickness 1.50 mm |
1610 °F @Thickness 0.0591 in |
GWFI; IEC 60695-2-12 |
Covestro Makrolon® ET3117 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc.. |
|||
Glow Wire Test | 875 °C @Thickness 1.50 mm |
1610 °F @Thickness 0.0591 in |
GWIT; IEC 60695-2-13 |
Covestro Makrolon® ET3117 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc.. |
|||
Glow Wire Test | 875 °C @Thickness 0.750 mm |
1610 °F @Thickness 0.0295 in |
GWIT; IEC 60695-2-13 |
Covestro Makrolon® ET2613 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• Medium vi.. |
|||
Glow Wire Test | 875 °C @Thickness 1.50 mm |
1610 °F @Thickness 0.0591 in |
GWIT; IEC 60695-2-13 |
Covestro Makrolon® ET3127 Polycarbonate Makrolon® polycarbonate resinMain characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characterist.. |
|||
Glow Wire Test | 875 °C @Thickness 2.00 mm |
1610 °F @Thickness 0.0787 in |
GWIT; IEC 60695 |
Eurotec® Tecopet® PT70 KK45 PET, 45% glass fiber/mineral reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Glow Wire Test | 875 °C @Thickness 2.00 mm |
1610 °F @Thickness 0.0787 in |
GWIT; IEC 60695 |
Eurotec® Tecotek® PC43 GR30 BK002 PC, 30% glass fiber reinforced, black Information provided by Eurotec® |
|||
Glow Wire Test | 875 °C @Thickness 0.400 mm |
1610 °F @Thickness 0.0157 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri.. |
|||
Glow Wire Test | 875 °C @Thickness 0.710 mm |
1610 °F @Thickness 0.0280 in |
Ignition Temp; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla.. |
|||
Glow Wire Test | 875 °C @Thickness 3.00 mm |
1610 °F @Thickness 0.118 in |
GWIT; IEC 60695-2-13 |
Covestro Makrolon® LED2643 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• LED lighting, optics, .. |