Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 8.0 MPa | 130 - 150 °C | 266 - 302 °F | Injection; ISO 75-C |
Raschig Group 2572 AMC Glass fiber reinforced Polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, good abrasion stability, high flame retardance in combin.. |
|||
Deflection Temperature at 8.0 MPa | 130 - 150 °C | 266 - 302 °F | Injection; ISO 75-C |
Raschig Group 5562 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Deflection Temperature at 8.0 MPa | 130 - 150 °C | 266 - 302 °F | ISO 75-C |
Raschig Group MELOPAS® 156 MF Melamine Glass fiber reinforced Melamine molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 200.. |
|||
Deflection Temperature at 8.0 MPa | 130 - 178 °C | 266 - 352 °F | Average value: 147 °C Grade Count:7 |
Overview of materials for Phenolic, Novolac, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral Filled". Each property range of values reported is minimum and maximum values.. |
|||
Deflection Temperature at 8.0 MPa | 130 °C | 266 °F | ISO 75-2 |
Hexion Bakelite™ PF 2736 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed
&nbs Phenolic molding compound, inorganically/organically filled, increased tracking resistance, UL listed molding compound 0.46 mm/V-0 (BK, Suffix "H"), 0.81 mm/V-0 (NC, GN, BK), 1.5 mm/V-0 (ALL).Applic.. |
|||
Deflection Temperature at 8.0 MPa | 130 °C | 266 °F | ISO 75-2 |
Hexion Bakelite™ PF 7400 Phenolic Formaldehyde Resin, High Mechanical Strength
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fiber flakes, high notched impact strength.Application areas: Moldings for higher mechanical strain, e.g. power plugs high volta.. |
|||
Deflection Temperature at 8.0 MPa | 130 °C | 266 °F | ISO 75-1/-2 |
Lanxess Pocan® B 3225 XF 000000 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding, improved flowability |
|||
Deflection Temperature at 8.0 MPa | 130 °C | 266 °F | ISO 75-1/-2 |
Lanxess Pocan® B 4235 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant |
|||
Deflection Temperature at 8.0 MPa | 130 °C | 266 °F | ISO 75-1/-2 |
Lanxess Pocan® B 4235 Z 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant, impact modified |
|||
Deflection Temperature at 8.0 MPa | 130 - 150 °C | 266 - 302 °F | ISO 75 C |
Vyncolit 4221 XB Novolac Phenolic Mineral and organic filled phenolic molding compound with good mechanical properties.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Deflection Temperature at 8.0 MPa | 130 - 150 °C | 266 - 302 °F | ISO 75 C |
Vyncolit 4451 XB Novolac Phenolic Organic and mineral filled phenolic molding compound with excellent mechanical properties (highest notched impact strength).USES: Fuse holders, brush holders, circuit breakers, automotive ignition a.. |
|||
Deflection Temperature at 8.0 MPa | 130 - 150 °C | 266 - 302 °F | ISO 75 C |
Vyncolit 2530 W Novolac Phenolic Mineral and organic filled phenolic molding compound with excellent thermal properties.USES: Lamp sockets, special lamp holders, pan handles and knobs.Information provided by Vyncolit, a Sumitomo Ba.. |
|||
Deflection Temperature at 8.0 MPa | 130 - 150 °C | 266 - 302 °F | ISO 75 C |
Vyncolit 2723 W Novolac Phenolic Mineral and organic filled phenolic molding compound with excellent mechanical, thermal and dielectric properties. I2/FO classified under NF F 16-101 (Fire & Smoke classification).USES: Circuit bre.. |
|||
Deflection Temperature at 8.0 MPa | 130 - 150 °C | 266 - 302 °F | ISO 75 C |
Vyncolit 2920 W Novolac Phenolic Mineral and organic filled molding compound with good dimensional stability and heat resistance.USES: Carburettor and intake manifold thermal insulator.Information provided by Vyncolit, a Sumitomo B.. |
|||
Deflection Temperature at 8.0 MPa | 130 °C | 266 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® BG-40 HM PA6-GF40 Product description: Grilon BG-40 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 40% glass fibers. Grilon BG-40 HM has the following important prop.. |
|||
Deflection Temperature at 8.0 MPa | 130 °C | 266 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® LVX-50H black 9230 PA12-GF50 Product description: Grilamid LVX-50H black 9230 is a 50% glass fiber reinforced, heat stabilized polyamide 12. Special characteristics of this injection molding product are: Very high stiffness and.. |
|||
Deflection Temperature at 8.0 MPa | 130 °C | 266 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® LVX-50H nat PA12-GF50 Product description: Grilamid LVX-50H natural is a 50% glass fiber reinforced, heat stabilized polyamide 12. Special characteristics of this injection molding product are: Very high stiffness and st.. |
|||
Deflection Temperature at 8.0 MPa | 130 °C | 266 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® TSC-30/4 LF 15 black 9832 PA666-(CF+Z)45 Product description: Grilon TSC-30/4 LF 15 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% carbon fibers and 15% of a combination of PTFE and silicone oil. Grilon .. |
|||
Deflection Temperature at 8.0 MPa | 130 °C | 266 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® TSG-30/4 FA PA666-GF30 Information provided by EMS Grivory |
|||
Deflection Temperature at 8.0 MPa | 130 °C | 266 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® TSG-30/4 H black 9836 PA666-GF30 Information provided by EMS Grivory |
|||
Deflection Temperature at 8.0 MPa | 130 °C | 266 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® TSG-30/4 H black 9839 PA666-GF30 Information provided by EMS Grivory |
|||
Deflection Temperature at 8.0 MPa | 130 °C | 266 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® LBV-65H FWA black 9225 PA12-GF65 Product description: Grilamid LBV-65H FWA black 9225 is a 65% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features High stiffness combined.. |
|||
Deflection Temperature at 8.0 MPa | 130 °C | 266 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® LBV-65H FWA nat PA12-GF65 Product description: Grilamid LBV-65H FWA natural is a 65% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w.. |
|||
Deflection Temperature at 8.0 MPa | 130 - 150 °C | 266 - 302 °F | ISO 75 C |
Vyncolit 3520 CG Novolac Phenolic Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par.. |
|||
Deflection Temperature at 8.0 MPa | 130 °C | 266 °F | ISO 75-2 |
Hexion Bakelite™ PF 2836 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed
&nbs Phenolic molding compound, inorganically/organically filled, increased heat resistance, increased tracking resistance, low shrinkage and post shrinkage, improved electrical properties, UL listed mol.. |