Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 62.2 °C | 144 °F | ASTM D648 |
Nylene® 9110 Unfilled Nylon 6/10 Description: Nylene® 9110 is an unfilled specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ASTM D648 |
Nylene® NX4301 Nylon 6, Extrusion Grade Dry as molded. Extrusion grade. Nylene NX4301 is a high viscosity, UV stabilized extrusion grade nylon resistant to degradation by ultraviolet light. The elevated quality of UV resistance is attri.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPC K5025 PP, Mineral Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPC T25020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ASTM D648 |
North Wood Plastics 60 PP + UNIFILL (20% Wood Fiber) Data provided by North Wood Plastics, Inc. UNIFILL-60 is a general purpose polyolefin compound compatible in both PP and HDPE. It is a masterbatch with 60% high quality pine wood flour filler. It.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C @Thickness 3.18 mm |
144 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Cellular E8202 Polyvinyl Chloride, Rigid (PVC, Rigid) All physicals were measured on an actual extruded part of a shutter profile.High rate inward foam applications.Density range .55-.70.Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C @Thickness 3.20 mm |
144 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP FARADEX PS003E PA 6 (Asia Pacific) LNP* Faradex* PS003E is a compound based on Nylon 6 resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ISO 75-1,-2 |
Gromax BTE30-DN00N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Thermocomp FX05032 PE (Europe-Africa-Middle East) LNP* THERMOCOMP* FX05032 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added features include : Foaming Agent for Polyolefins.This data was supplied by SABIC-IP for t.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ISO 75-2 |
Borealis PS65C40 Polypropylene Compound, Mineral Filled PS65C40 is a 40% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives a good surface quality and.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ASTM D648 |
A. Schulman POLYFORT™ PP 3726 Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ASTM D648 |
A. Schulman PP 3490-01G Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3490-01G Natural is a homopolymer for extrusion and compounding applications. This material can also be used as a carrier resin for color concentrates. ApplicationPP 349.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ASTM D648 |
A. Schulman POLYFORT™ PP 3726 Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ASTM D648 |
A. Schulman PP 1102-01 Polypropylene General Purpose, Molding Grade Polypropylene DescriptionPolypropylene PP 1102-01 is a general purpose, molding grade with UL 94 HB approval for use in large and thin wall applications. ApplicationPolypropylene PP 1102-01 meets FDA Regulation.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ASTM D-648-92 |
Lubrizol Stat-Rite® X5166 Static Dissipative Polystyrene Compound Stat-Rite® X5166 is a static dissipative, High-Impact Polystyrene alloy. Stat-Rite® X5166 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, perm.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ASTM D648 |
Eastman Amphora™ AM1800 3D Polymer Eastman Amphora™ 3D polymer is a low-odor, styrene-free choice that was developed for 3D Printing applications. With Amphora, makers can create items that are more functional, durable, efficient, a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ASTM D648 |
Eastman Drystar 0603 Copolyester This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ASTM D648 |
Eastman Eastar MN052 Polyester, Natural Eastar polyester MN052 is a thermoplastic condensation homopolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystalliz.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ASTM D648 |
Eastman Eastar GN046 Copolyester, Natural Eastar Copolyester GN046 is a very high melt strength copolyester targeted for extrusion blow molding applications. Blow molding of large parts (up to several pounds) are possible with this material.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.2 °C | 144 °F | |
Aclo Accutech Polypropylene Homopolymer HP0339C40L1 Calcium Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ISO 75-2/AF |
Addiplast Addilene H 140 Polypropylene Homopolymer Unreinforced, low flow for injection and extrusion, very translucentInformation provided by Addiplast. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ISO 75-2/AF |
Addiplast Addilene H 210 G20 Polypropylene Homopolymer Glass bead reinforced, improved stiffness and dimensional stabilityInformation provided by Addiplast. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ISO 75-2/AF |
Addiplast Addilene J 220 M20 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ASTM D648 |
3D Systems Accura® Amethyst™ Plastic for Viper™ SLA® Systems Optimized for the rapid and automated production of patterns and master molds for jewelry manufacturing. For use with Viper™ SLA® systems.ApplicationsPatterns for use with low and high vulcanizing.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.2 °C | 144 °F | |
Aclo Accutech Polypropylene Homopolymer HP0339M10L Mica Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.2 °C | 144 °F | |
Aclo Accutech Polypropylene Homopolymer HP0339T30L Talc Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ISO 75-2/AF |
Addiplast Addilene J 290 M20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ISO 75-2/AF |
Addiplast Addilene J 520 T30 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.0 °C | 144 °F | ASTM D648 |
A. Schulman PP 1102-01 Polypropylene General Purpose, Molding Grade Polypropylene DescriptionPolypropylene PP 1102-01 is a general purpose, molding grade with UL 94 HB approval for use in large and thin wall applications. ApplicationPolypropylene PP 1102-01 meets FDA Regulation.. |