Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 62.8 °C | 145 °F | ASTM D648 |
RheTech Products CC40P100-00EG 40% Calcium Carbonate Reinforced Polypropylene, Natural, Extrusion Grade Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.8 °C | 145 °F | ASTM D648 |
RheTech Products T15P100-00 12% Talc Reinforced Polypropylene, Natural Applications: Component housingConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.8 °C | 145 °F | ASTM D648 |
Polymer Resources NY6-IM1-[color]H Nylon, Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | |
Solvay Specialty Polymers Halar® 300 ECTFE Fluoropolymer
(discontinued **) Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.8 °C | 145 °F | ASTM D648 |
Fiberfil® PP-61/VO Polypropylene Copolymer, Flame Retardant, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRICOMP RP004 PA 66 LNP LUBRICOMP* RP004 is a compound based on Nylon 66 resin containing 20% PTFE/Silicone. Added features of this material include: Wear Resistant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRICOMP WL0049 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WL0049 is a compound based on Polybutylene Terephalate resin containing PTFE and Flame Retardant. Added features include: Internally Lubricated, Flame Retardant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C @Thickness 3.20 mm |
145 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRILOY RX99650 PA 66 (Europe-Africa-Middle East) LNP LUBRILOY* RX99650 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.8 °C | 145 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® PA6/6 FR 346 RD Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Flame Retardant, Heat Stabilized and LubricatedAppearance: RedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C @Thickness 3.20 mm |
145 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP MB006HS PP LNP* THERMOCOMP* MB006HS is a compound based on Polypropylene resin containing 30% Glass Bead. Added features of this material include: Heat Stabilized, Healthcare. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Thermocomp MX05039 PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MX05039 is a compound based on Polypropylene resin containing Mineral, colorant. Added features include : Heat- Stabilized, UV - Stabilized.This data was supplied by SABIC-IP for th.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.8 °C | 145 °F | ASTM D648 |
Washington Penn High Modulus Polypropylene Copolymer 15% Mica Filled Mica-filled polypropylene compounds provide the best strength and modulus of any of the particulate fillers which results in an outstanding balance of properties. Mold shrinkage is similar to ABS a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 62.8 °C | 145 °F | ASTM D648 |
Westlake Plastics ECTFE Film Made from HALAR® Ethylene-chlorotrifluoroethylene Resin Excellent purity. Excellent chemical resistance. Low permeability. Excellent abrasion resistance. Excellent temperature resistance.Halar® is a trade name of Solvay Solexis, Inc. Information p.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1477 Mineral Filled, General-Purpose Polypropylene DescriptionPolyfort® FPP 1477 is a 20% mineral filled, general-purpose polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 2496 Injection Molding Grade, Mineral Fortified Polypropylene DescriptionPolyfort® FPP 2496 is an injection molding grade mineral fortified and impact enhanced polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ASTM D648 |
Eastman Eastar CN015 Copolyester, High Flow Grade with Mold Release Applications:CompactsCosmetic jar capsCosmetic jarsCosmetics/personal care packagingFragrance capsFragrance packagingLip gloss containersLipstick containersPersonal care bottlesKey Attributes:Abilit.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | |
Eastman Eastar EN058 PET Copolymer ISO data as provided by the manufacturer, Eastman Chemical |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ASTM D648 |
Eastman Eastar MN200 Copolyester Eastar Copolyester MN200 is an amorphous copolyester with excellent flow characteristics as well as radiation resistance and chemical resistance.Applications/UsesMedical |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | Flatw 80x10x4, sp=64 mm; ISO 75/Af |
Eurostar Starpylen MX05039 PP, Mineral Filled, Injection Molding Starpylen MX05039 is a Mineral Filled Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ISO 75-2/AF |
Addiplast Addilene H 410 Polypropylene Homopolymer UnreinforcedInformation provided by Addiplast. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ISO 75 |
Ascend Performance Materials Vydyne® 47 Nylon 66, DAM Vydyne® 47 Nylon resins are general purpose polyamide, impact modified grades. They are available in natural, black and heat stabilized for improved resistance to elevated temperatures. The heat st.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | Unannealed; ISO 75-2/A |
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ASTM D648 |
Ashley Polymers Ashlene® 527LDMS Nylon 66 A very high impact Nylon 66 with Molybdenum disulfide designed to combine high impact with a reduced co-efficient of friction.Data provided by the manufacturer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ASTM D648 |
A. Schulman ComAlloy Comtuf® 109 Polypropylene, Mineral Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.40% Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ASTM D648 |
Ashley Polymers Ashlene® 830L Nylon 6 Basic Nylon 6, medium viscosity, lubricated.Data provided by the manufacturer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ASTM D648 |
Ashley Polymers Ashlene® 835 Nylon 6 Basic Nylon 6 high viscosity, for coating and laminating applications, FDA approved.Data provided by the manufacturer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPH TS4020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 2496 Injection Molding Grade, Mineral Fortified Polypropylene DescriptionPolyfort® FPP 2496 is an injection molding grade mineral fortified and impact enhanced polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 63.0 °C | 145 °F | Unannealed; ISO 75-2/A |
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, DAM Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |