Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 226 °C @Thickness 3.20 mm |
439 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 (Europe-Africa-Middle East) LNP* Konduit* RTF2B is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 226 °C | 439 °F | ASTM D648 |
Covestro Petlon® DP3-1027 Semi-Crystalline PET, 45% Glass Fiber
(discontinued **) Characteristics: General Purpose: Good Strength, High Rigidity and Heat ResistanceApplications: Automotive Valve Covers, Pump Components and PulleysProcessing: Injection Molding (Melt Temperature: 4.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 226 °C | 439 °F | DIN 53461 |
Polyram PE322G22 PET, 22% Glass Fiber
(discontinued **) 22% Glass fiber reinforced, flame retardant PET for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 226 °C @Thickness 3.20 mm |
439 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 LNP* KONDUIT* RTF2B is a compound based on Nylon 66 resin containing 10% Glass Fiber, 55% Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 226 °C @Thickness 3.20 mm |
439 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 (Asia Pacific) LNP* Konduit* RTF2B is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 226 °C | 439 °F | ISO 75-1,-2 |
Gromax CFG35-R113N1 Nylon 6 36% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 226 °C | 439 °F | ISO 75/Af |
Solvay TECHNYL® A 30 H1 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 30H1 V30 is a brominated flame retardant polyamide 66, reinforced with 30% of glass fiber, for injection molding. This product is available in natural & black color.Benefi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 226 °C @Thickness 3.20 mm |
439 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP RF0039S PA 66 LNP THERMOCOMP* RF0039S is a compound based on Nylon 66 resin containing 15% Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 226 °C | 439 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP Thermocomp RF004S PA 66 LNP* Thermocomp* RF004S is a Nylon 6/6 containing Glass Fiber. Characteristics are Heat Stabilized.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 226 °C | 438 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PBT G/CF30 15% Glass/Carbon Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Carbon Fiber Reinforcement, 15% Filler by WeightAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 226 °C | 439 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP RF006EUC PA 66 LNP* THERMOCOMP* RF006EUC is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include Easy Molding, UV Stabilized. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 226 °C | 439 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP RFB44XE PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RFB44XE is a compound based on Nylon 66 resin containing Glass Fiber, Glass Bead. Added features of this material include: Easy Molding. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 226 °C @Thickness 3.20 mm |
439 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP RX93402 PA 66 LNP THERMOCOMP* RX93402 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 226 °C | 438 °F | ASTM D648 |
A. Schulman SCHULADUR® B GF30 30% Glass Fiber Reinforced PET Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 226 °C | 439 °F | ASTM D648 |
Plenco 6401 Phenolic, Granular, Compression Molded PLENCO 06401 is a glass fiber and mineral filled two-stage phenolic molding compound. UL recognized under component file E40654. 06401 is available in black.Information supplied by Plenco. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 226 °C | 439 °F | ASTM D648 |
Plenco 6553 Phenolic, Granular, Compression Molded Two-Stage Phenolic. PLENCO 06553 is a phenolic molding compound, formulated specifically for automotive brake pistons. 06553 exhibits excellent dimensional stability, and resistance to brake fluids.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 226 °C | 438 °F | ASTM D648 |
A. Schulman SCHULADUR® B GF30 30% Glass Fiber Reinforced PET Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 226 °C | 438 °F | ASTM D648 |
A. Schulman SCHULADUR® B GF30 30% Glass Fiber Reinforced PET Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 226 °C | 438 °F | ASTM D648 |
A. Schulman SCHULADUR® B GF30 30% Glass Fiber Reinforced PET Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 226 °C | 438 °F | ASTM D648 |
A. Schulman SCHULADUR® B GF30 30% Glass Fiber Reinforced PET Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 226 °C | 439 °F | ASTM D648 |
Plenco 1506 Polyester, Briquette, Injection Molded PLENCO 01506 is a mineral and cellulose filled granular polyester molding compound, with glass fiber reinforcement for improved mechanical strength properties. 01506 offers excellent electrical prop.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 226 °C | 438 °F | ASTM D648 |
A. Schulman SCHULADUR® B GF30 30% Glass Fiber Reinforced PET Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 226 °C | 439 °F | ISO 75-1,-2 |
Gromax CFG35-R113N1 Nylon 6 36% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |