Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 288 °C | 550 °F | Unannealed; ISO 75-2/A |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Dry) Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 288 °C | 550 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PEEK CF20 TL15 HF 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: High Flow and LubricatedInformation provided by TP Composi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 288 °C | 550 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PEEK GF30 HF 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: High FlowInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 288 °C | 550 °F | ASTM D648A |
Sumitomo Bakelite North America 2-530 Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Am.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 288 °C | 550 °F | Annealed, 0.125 in bars; ASTM D648 |
PolyOne Edgetek® AM 33 GF/000 L HS Black Polyphthalamide (PPA), Glass Filled
(discontinued **) Description/Features:Heat StabilizedBlackEnhanced LubricationGlass Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 288 °C | 550 °F | Unannealed; ASTM D648 |
PolyOne Edgetek® AM-30GF/000 Polyphthalamide (PPA), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 288 °C | 550 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA4/6 GF30 FR HS L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Flame Retardant and Lu.. |