Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C @Thickness 3.20 mm |
289 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Lexan® HPH4504 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C @Thickness 3.20 mm |
289 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® HPH4504 PPC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C @Thickness 3.20 mm |
289 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Asia Pacific) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C @Thickness 6.40 mm |
289 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Lexan® LGK5030 PC (Asia Pacific) Glass reinforced. Flame retardant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C @Thickness 3.20 mm |
289 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP DFL34 PC LNP LUBRICOMP* DFL34 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C @Thickness 3.20 mm |
289 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubrica.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C @Thickness 3.20 mm |
289 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP DFL14 PC (Asia Pacific) LNP* LUBRICOMP* DFL14 is a compound based on Polycarbonate resin containing PTFE, Glass Fiber. Added features of this material include: Internally Lubricated. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP STAT-KON DE003Z PC (Asia Pacific) LNP STAT-KON* DE003Z is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP STAT-KON DE0069F PC LNP* STAT-KON* DE0069F is a compound based on Polycarbonate resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Superior Molding. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP STAT-KON DEF42 PC LNP STAT-KON* DEF42 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP STAT-KON DX06500 PC (Asia Pacific) LNP* Stat-kon* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C @Thickness 3.20 mm |
289 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP DF0049 PC LNP THERMOCOMP* DF0049 is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP DF006 PC (Europe-Africa-Middle East) LNP* Thermocomp* DF1006 is a compound based on Polycarbonate resin containing Glass Fiber. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | Annealed; ISO 75-2/A |
Styron CALIBREâ„¢ 200-6 Polycarbonate Resin Overview: CALIBREâ„¢ 200-6 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistance.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | Annealed; ISO 75-2/A |
Styron CALIBREâ„¢ 301-6 Polycarbonate Resin Overview: CALIBREâ„¢ 300-6 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet applic.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | Annealed; ISO 75-2/A |
Styron CALIBREâ„¢ 303V-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300V-10 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, optical clarity and meets UL94 V-2 rating. CALIBRE 300V series products are avai.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP STAT-KON DEL22P PC (Asia Pacific) LNP STAT-KON* DEL22P is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | Annealed; ISO 75-2/B |
Styron CALIBREâ„¢ 302-6 Polycarbonate Resin Overview: CALIBREâ„¢ 300-6 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, and optical clarity as well as high melt strength for blow molding and sheet appli.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | Annealed; ISO 75-2/A |
Styron CALIBREâ„¢ 303-6 Polycarbonate Resin Overview: CALIBREâ„¢ 300-6 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet applic.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | Heat Distortion temperature |
Cosmic Plastics ID-50 Dacron Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | ASTM D648 |
A. Schulman ComAlloy® E-17036 Glass Fiber Reinforced High Heat Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | 0.125";; ASTM D648 |
Diamond Polymers NPP25-0303 GF20 20% Glass Filled Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | ASTM D648 |
E-Polymers TEKANATE™ G710 , 10% Glass Fiber Reinforced Poly Carbonate 10% Glass Fiber reinforcedInformation provided by E-Polymers Co. Ltd. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | |
Aclo Accutech Polypropylene Homopolymer HP0339G30CL Glass Reinforced Coupled |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | ASTM D648 |
Ashley Polymers Ashlene® P1525B Polycarbonate A rigid flame retardant black polycarbonate, for applications requiring superior dimensional stability and overall toughness.Data provided by the manufacturer |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | ASTM D648 |
A. Schulman ComAlloy Hiloy® 109 Polypropylene, Glass/Mineral Reinforced, Chemically Coupled Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | ASTM D648 |
A. Schulman ComAlloy Hiloy® 514 Polycarbonate, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | ASTM D648 |
A. Schulman ComAlloy Hiloy® 518 Polycarbonate, Carbon Fiber Reinforced Data provided by the manufacturer, ComAlloy International Company.40% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C @Thickness 3.20 mm |
289 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36HL PC LNP LUBRICOMP* DFL36HL is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractable, Healthcare. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 143 °C | 289 °F | ASTM D648 |
PolyOne Stat-Tech™ MP-25NCF/000 Modified PPO - 25% Nickel Coated Graphite Fiber
(discontinued **) Data provided by PolyOne. |