Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 316 °C | 600 °F | ASTM D648 |
Ensinger Sintimid™ V Unfilled Polyimide (PI)
(discontinued **) SINTIMID™ V polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an idea choice for the most demanding applications. SINTIMID™ V.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | >= 316 °C | >= 600 °F | ASTM D648 |
Ensinger Sintimid™ V 15% graphite Polyimide (PI)
(discontinued **) SINTIMID™ V polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an idea choice for the most demanding applications. SINTIMID™ V.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | >= 316 °C | >= 600 °F | ASTM D648 |
Ensinger Sintimid™ V 40% graphite Polyimide (PI)
(discontinued **) SINTIMID™ V polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an idea choice for the most demanding applications. SINTIMID™ V.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 316 °C | 600 °F | |
Greene Tweed WR™ 300 PEEK, Carbon Filled WR®300 is a carbon-fiber reinforced compression molded PEEK often selected by pump manufacturers and users for pump bushings and case or impeller wear rings. Maximum service life is achieved in .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 316 °C | 601 °F | ASTM D648 |
Saint-Gobain Meldin® 5055 Thermoplastic Bearing Material General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | >= 316 °C | >= 600 °F | |
Bulk Molding Compounds BMC 615 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 615 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ext.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 316 °C | 601 °F | ASTM D648 |
Saint-Gobain Meldin® 5330 Thermoplastic Bearing Material General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin.. |