Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 398 °F
Polymer Property :
Deflection Temperature at 1.8 MPa (264 psi) =
398 °F
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
203
°C
398
°F
ASTM D648
Nylene® 9110 G43 , 43% Glass Reinforced Nylon 6/10
Description: Nylene® 9110 G43 is a 43% glass fiber reinforced specialty nylon.