Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 525 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 274 °C
525 °F
ASTM D648A
Sumitomo Bakelite North America RX® 2-501N Mineral Filled Diallyl Phthalate
Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Conforms with the requirements of ASTM D5948..
Deflection Temperature at 1.8 MPa (264 psi) 274 °C
525 °F
ASTM D648A
Sumitomo Bakelite North America RX® 3-2-520F-P Short-Glass Reinforced Diallyl Phthalate
Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SI..
Deflection Temperature at 1.8 MPa (264 psi) 274 - 290 °C
525 - 554 °F
Average value: 284 °C Grade Count:10
Overview of materials for Nylon 46, Lubricated + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Lubricated + Glass Fiber Reinforced". Each property range of values reported is minimum and ma..
Deflection Temperature at 1.8 MPa (264 psi) 274 °C
525 °F
ASTM D648A
Sumitomo Bakelite North America FS-6 CAF Mineral Filled Diallyl Phthalate
Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type MI..