Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 288 °C | 550 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA4/6 GF45 HS BK 45% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 45% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackTPCI# 9627150Informat.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 288 °C | 550 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PEEK CF20 TL15 HF 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: High Flow and LubricatedInformation provided by TP Composi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 288 °C | 550 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PEEK CF40 HF 40% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightFeatures: High FlowInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 288 °C | 550 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PEEK GF30 HF 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: High FlowInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 288 °C | 550 °F | ASTM D648A |
Sumitomo Bakelite North America 3-2-530 Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North A.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 288 °C | 550 °F | Unannealed; Flatwise; ISO 75-2/A |
Solvay Specialty Polymers Amodel® A-6135 NL Polyphthalamide (PPA), 35% Glass Fiber Reinforcement
(discontin Amodel A-6135 NL polyphthalamide (PPA), a 35% glass reinforced, high-glow, non-lubricated, hot-water moldable resin specially designed for laser welding. The black version is a laser absorber, and t.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 288 °C | 550 °F | Unannealed; ASTM D648 |
PolyOne Edgetek® AM-30GF/000 Polyphthalamide (PPA), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 288 °C | 550 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA4/6 GF30 FR HS L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Flame Retardant and Lu.. |