Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C @Thickness 3.20 mm |
178 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycolac® MG29 ABS Super high impact ABS. Good low temperature toughness. High gloss. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C @Thickness 3.20 mm |
178 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycolac® MG29 ABS (Asia Pacific) Super high impact ABS. Good low temperature toughness. High gloss. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C | 178 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Cycolac® MG38 ABS Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C | 178 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Cycolac® MG38 ABS (Europe-Africa-Middle East) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C | 178 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Cycolac® MG47 ABS Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C | 178 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Cycolac® MG47 ABS (Europe-Africa-Middle East) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C @Thickness 6.40 mm |
178 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C @Thickness 3.20 mm |
178 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS (Asia Pacific) Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C @Thickness 3.20 mm |
178 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS (Europe-Africa-Middle East) Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C @Thickness 3.20 mm |
178 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics GELOY FXW749SK ASA Sparkle VisualFx ASA Resin - Weatherable |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C | 178 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYlux 3809S FR PC/PBT-Blend, Flame Retardant Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C | 178 °F | 120°C/h; ASTM D 648 |
Polimeri Europa Edistir RCL 600 Polystyrene
(discontinued **) Special medium impact polystyrene extrusion grade exhibiting very high gloss. This grade should be used where is required an excellent surface finish. It can be directly extruded in foils and sheets.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C | 178 °F | ASTM D648 |
North Wood Plastics PS with 40% Wood Fiber Data provided by North Wood Plastics, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C | 178 °F | ISO 75-1,-2 |
Inno-Comp INNOPOL® CS 1-6140 N 40% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-6140 N is a 40% talc-filled polypropylene homopolymer compound /PP-H TD40 (ISO 1043)/.INNOPOL® CS 1-6140 N is developed for producing injection molded components for household eq.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C @Thickness 6.35 mm |
178 °F @Thickness 0.250 in |
ASTM D648 |
IRPC Polimaxx Polene 121PC Styrene Acrylonitrile APPLICATIONS: INJECTION MOLDING, HOUSEHOLD PRODUCTS : SANITARY WARE, AUTOPART APPLICATION : LAMP ELECTRICAL APPLIANCES : ELECTRICAL FAN |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C @Thickness 6.40 mm |
178 °F @Thickness 0.252 in |
ASTM D648 |
Kingfa PBT-RG002 Flame Retardant PBT Features:Flame retardantGood chemical resistanceOutstanding surfaceEasy processingHigh impactApplications:Injection moldingConnectors, terminal blocksRelay, switchBobbinsPlugsE & E partsInformation .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C | 178 °F | unannealed; ASTM D648 |
KKPC Kuhmo HI 450PG High Gloss HIPS Common Uses: Monitor swivels, washers.HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between impact-resistance and heat-resistance.Data pr.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C | 178 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS LNP* STAT-LOY* A30009 is a compound based on ABS. Added features of this material include: Antistatic, Flame Retardant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C @Thickness 6.40 mm |
178 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® SD-0170 F ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C @Thickness 6.40 mm |
178 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® VE-0813 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C @Thickness 6.40 mm |
178 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® VE-0812 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C | 178 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Valox® V3903WX PBT+PC (Asia Pacific) Unreinforced fllame retardant PBT/PC blends with good chemical resistance and low temperature impact, UV stablized |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C | 178 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C | 178 °F | ASTM D648 |
Supreme Petrochem SC 206 General Purpose Polystyrene CharacteristicsGood flow grade with clarity & shine Improves aesthetics of final product Processing MoldingApplications Crystal ware, paper weights, house ware Beads, Bangles, gift articles, trays,.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C | 178 °F | ASTM D648 |
Supreme Petrochem SP 562 Flame Retardant Polystyrene Characteristics Very good flow properties Free of DBDPO, PBDE & TBBA, complies with ROHS directive of EU Low specific gravity Processing Injection moldingApplications Large size T.V. Cabinets Aud.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C | 178 °F | ASTM D648 |
Eastman Tritan MX730 Copolyester Eastman Tritan Copolyester MX730 is an amorphous product with excellent appearance and clarity. Eastman Tritan Copolyester MX730 is a high flow medical grade of Eastman Tritan that has viscosity re.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C | 178 °F | ASTM D648 |
Eastman Tritan MX731 Copolyester Eastman Tritan Copolyester MX731 is an amorphous product with excellent appearance and clarity. Eastman Tritan Copolyester MX731 is a high flow medical grade of Eastman Tritan that has viscosity re.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C | 178 °F | ASTM D648 |
Eastman Tritan TX1501HF Copolyester Eastman Tritan TX1501HF is a high flow grade of Eastman Tritan. Eastman Tritan TX1501HF has viscosity reductions of 40-50% relative to Eastman Tritan copolyester TX1001. Eastman Tritan copolyester.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C | 178 °F | annealed; ASTM D648 |
Kleerdex Kydex® 1900 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Mid-temperature aircraft gradeApplications: This sheet product is designed for use in small aircraft interiors but also is appropriate for other applications where higher in-service temperatures may.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C | 178 °F | ASTM D648 |
Supreme Petrochem SP 6605 Toughened Polystyrene Characteristics Excellent melt strength High stiffness Easy tearability Processing Extrusion Applications Suitable for thin film for candy wrap and window envelope Economic production of clear th.. |