Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ASTM D648 |
Plaskolite West Optix® CA-61 Clear UV General Purpose Acrylic Resin General purpose acrylic resin, injection molding and extrusion gradeApplications: A general-purpose acrylic resin designed primarily for injection molding. This resin offers a medium melt flow rate.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ASTM D648 |
Ineos Nova 474 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Custom ColorsApplications: Injection molding, Alternative to engineering resinsPerformance grades of polystyrene are engineered to have specific properties. These products can be custom colored. N.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 - 163 °C | 196 - 325 °F | Average value: 149 °C Grade Count:35 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | Unannealed; ASTM D648 |
PolyOne Edgetek® AS-10GF/000 NATURAL Acrylonitrile Butadiene Styrene (ABS) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C @Thickness 6.40 mm |
196 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical LUPOY GP5008A PC/ABS Description: Injection Molding, PC/ABS, General Purpose, High FlowApplication: Miscellaneous GoodsCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ASTM D648 |
Ineos Nova 3101 General Purpose Crystal Polystyrene Good balance of flow and set-up properties, Good crack resistanceApplications: Single service cutlery, Single service drinkware, Consumer electronic packagingExposure to gamma radiation in the 2.02-.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ISO 75A |
Lucite International Diakon® ST50G8 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C @Thickness 6.35 mm |
196 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
LG Chemical 92HR SAN Resin Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include automobile battery cases, water meter case.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ISO 75-1,-2 |
Ineos ABS Lustran® ABS 650 Injection Molding Grade Lustran® ABS 650 has high impact strength, high flow, and is injection molding grade. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C @Thickness 3.20 mm |
196 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP WL0049 PBT LNP* LUBRICOMP* WL0049 is a compound based on PBT containing 20% PTFE. Added features include: Wear Resistant, Flame Retardant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C @Thickness 3.20 mm |
196 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRILOY KL201 Acetal (Europe-Africa-Middle East) LNP LUBRILOY* KL201 is a compound based on Acetal resin containing PTFE, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Europe-Africa-Middle East) Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ISO 75 |
Styrolution Novodur® 530 ABS Novodur 530 is an extrusion grade optimized for sheet applications. It has high impact properties, high modulus and good thermoforming.Information provided by Styrolution |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C @Thickness 3.20 mm |
196 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP KZ004 Acetal Copolymer LNP THERMOCOMP* KZ004 is a compound based on Acetal Copolymer resin containing 20% Milled Glass. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C @Thickness 6.40 mm |
196 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® SP-0183 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C @Thickness 6.40 mm |
196 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Infino® HP-0500 ABS, Unreinforced Heat Resistant ABS material that can mainly be used for the exterior material of household appliances etc.Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C @Thickness 6.40 mm |
196 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® QU-0191S ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C @Thickness 6.40 mm |
196 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® ST-0185 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C @Thickness 6.40 mm |
196 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® SP-0183 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | 0.5 inch; ASTM D648 |
PlastxWorld CEVIAN® E11 Inherently Static Dissipative ABS These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | 0.25 inch; ASTM D648 |
PlastxWorld CEVIAN® LMB10 Laser Markable Grade ABS Black MarkingThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ISO 75-1,-2 |
Covestro Bayblend® FR3006 HF PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ISO 75-1,-2 |
Covestro Bayblend® FR3100 TV PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ISO 75-1/-2 |
DuPont Performance Polymers Delrin® 127UVE NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 127UVE NC010 (formerly DE20555) is a high viscosity acetal homopolymer with UV stabilizers with very low VOC emissions .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | annealed; ISO 75 |
Chi Mei Polylac® PA-765A ABS - Flame Retardant F.R. High Flow |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ISO 75 -1 & -2 flat |
Asahi Kasei Tenac®-C 4563 Copolymer Acetal Resin Weather-Resistant grade containing UV absorber and other additives for superior weathering abilityInformation provided by Asahi Kasei Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.0 °C | 196 °F | ASTM D648 |
Plaskolite West Optix® CA-61 General Purpose Acrylic Resin Injection Molding and Extrusion Grade Pellets. Good heat resistance, medium flow. |