Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 242 °C | 468 °F | at 760 mmHg |
LyondellBasell Glycol Ether DBA Diethylene glycol butyl ether acetate Information provided by Lyondell. |
|||
Boiling Point | 242 °C | 468 °F | at 760 mmHg |
LyondellBasell Propylene Carbonate Information provided by Lyondell. |
|||
Boiling Point | 242 °C | 468 °F | Initial; ASTM D86 |
ExxonMobil Solvesso™ 200 ND Aromatic Fluid Appearance: Transparent - Slight Yellow LiquidAvailability: Africa & Middle East, Europe, Asia Pacific, Central America, North America and South AmericaInformation provided by ExxonMobil |
|||
Boiling Point | 242 °C | 468 °F | |
BASF 2-Pyrrolidone Water Blend Formula: C4H7NOCAS: 7732-18-5Description: Pyrrolidone is a colorless to yellow liquid, with a faint amine-like odor. It is miscible in water.Synonyms: 2P water blend, Pyrrolidone, 2-Pyrrolidinone, 2.. |