Polymer Property : Flash Point = 15.6 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point 15.6 °C
60.0 °F
ASTM D56
Humiseal 1A20LSE Urethane Conformal Coating
Humiseal 1A20LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingMIL-I-46058C Approval pendingPasses ther..
Flash Point 15.6 °C
60.0 °F
ASTM D56
Humiseal 1A27LSE Urethane Conformal Coating
Humiseal 1A27LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingPasses thermal shock test (MIL-I-46058C)..
Flash Point 15.6 °C
60.0 °F
ASTM D56
Humiseal 1A33LSE Urethane Conformal Coating
Humiseal 1A33LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses ther..
Flash Point 15.6 °C
60.1 °F
HPC-3C; Seta
Lord Adhesives HPC-3C Fluoroelastomer Coating
LORD HPC-3B and HPC-3C are two-part, room temperature curing fluoroelastomer coatings which feature robust adhesion and exceptional mechanical properties. These coatings greatly enhance fuel and flu..
Flash Point 15.6 °C
60.1 °F
Seta
Lord Adhesives HPC-5B Hydrogenated Nitrile Butadiene Rubber Coating
LORD HPC-5B and HPC-5C are one-part, room temperature curing HNBR coatings which feature robust adhesion and exceptional mechanical properties. These coatings greatly enhance fluid and ozone resista..
Flash Point 15.6 °C
60.1 °F
Seta
Lord Adhesives HPC-5C Hydrogenated Nitrile Butadiene Rubber Coating
LORD HPC-5B and HPC-5C are one-part, room temperature curing HNBR coatings which feature robust adhesion and exceptional mechanical properties. These coatings greatly enhance fluid and ozone resista..
Flash Point 15.6 °C
60.1 °F
CC
LG Chemical Methyl Acrylate
Features: Low Color - Refining process are improved for produce the low color. Color is the main quality factor that influence the property of the final products. Low Acidity - Through the multistag..
Flash Point 15.6 °C
60.1 °F
HPC-3B; Seta
Lord Adhesives HPC-3B Fluoroelastomer Coating
LORD HPC-3B and HPC-3C are two-part, room temperature curing fluoroelastomer coatings which feature robust adhesion and exceptional mechanical properties. These coatings greatly enhance fuel and flu..
Flash Point 15.6 °C
60.1 °F
Closed cup
Dow Corning XIAMETER® PMCPOFX-0536 Fluid
Is chemically equivalent to DOW CORNING® 536 FLUID. 100 % active, amino methoxy functional polydimethylsiloxane.Information provided by Dow Corning
Flash Point 15.6 - 400 °C
60.1 - 752 °F
Average value: 323 °C Grade Count:93
Overview of materials for Thermoset Fluoroelastomer
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr..