Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | 300 °C | 572 °F | 5% weight loss; TGA; IPC-TM-650.2.4.24.6 |
Park Electrochemical Nelco® N4000-2 Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-2 is the most established material of Nelco’s product line. This multifunctional epoxy laminate and prepreg system has a long history of use and one of the broadest operating and .. |
|||
Decomposition Temperature | 300 °C | 572 °F | 1% mass loss, N2; TGA |
Solvay Specialty Polymers Halar® 1400LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**) Information provided by Solvay Specialty Polymers. |
|||
Decomposition Temperature | 300 - 350 °C | 572 - 662 °F | Thermal Stability via TGA : beginning - and at 1% weight loss in air |
Solvay Specialty Polymers Solef® 3108/0903 Anti-static PVDF Compound
(discontinued **) Key features of this grade: Anti-static, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crystall.. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultradur® S 4090 G2 10% Glass Filled PBT Description: Is a PBT + ASA, easy-flowing injection-molding grades with 10% glass fibers; for rigid, tough and dimensionally stable technical parts e. g. housings, consoles, contact carriers, covers.. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® A24 E 01 PA66 Information provided by BASF |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® A27 E PA66 Description: Ultramid® A27 E is a polyamide 66 grade for compounding.Information provided by BASF |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B36 LNV PA6 Information provided by BASF |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3EG6 LS BK 23189 30% Glass Filled PA6 (Dry) Information provided by BASF |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3EG7 35% Glass Filled PA6 (Conditioned) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3EG7 35% Glass Filled PA6 (Dry) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3EG7 BK 00564 35% Glass Filled PA6 (Conditioned) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B40 LN PA6 Description: Ultramid® B40 LN is a polyamide 6 grade of high viscosity that is well suited for the production of blown and cast film. Clarity and thermoformability are enhanced by the incorporation.. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® C33 L PA6/66 Description: Ultramid® C33 L is a lubricated copolyamide 6/66 grade of intermediate viscosity for the production of mulitlayer film. Ultramid® C33 L is well suited for the production of nonsymmetr.. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3GK24 BK 00564 10/20% Glass/Glass Bead Filled PA6 (Conditioned) Description: combined 10% glass-fiber and 20% glass-bead reinforced injection-molding grade for technical articles of very good dimensional stability, for instance, vehicle ash tray housings and ele.. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3GK24 BK 00564 10/20% Glass/Glass Bead Filled PA6 (Dry) Description: combined 10% glass-fiber and 20% glass-bead reinforced injection-molding grade for technical articles of very good dimensional stability, for instance, vehicle ash tray housings and ele.. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Conditioned) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3WG6 HP BK 23210 30% Glass Filled PA6 (Conditioned) Description: 30% Glass fiber reinforced and heat aging resistant injection molding grade with enhances flowability used e.g. for automobile manifold.Information provided by BASF |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3WG6 HP BK 23210 30% Glass Filled PA6 (Dry) Description: 30% Glass fiber reinforced and heat aging resistant injection molding grade with enhances flowability used e.g. for automobile manifold.Information provided by BASF |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® C33 PA6/66 Description: Ultramid® C33 is a copolyamide 6/66 grade of intermediate viscosity for the production of mulitlayer film and monofilaments. Ultramid® C33 is well suited for the production of nonsymm.. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® Seal-Fit PA6/66 (Dry) Description: Transparent, tough, amorphous copolyamide for injection molding, specially developed for tight overmoulding of metal inlays.Information provided by BASF |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3M6 Grey 22319 Q94 30% Mineral Filled PA6 (Conditioned) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3UG4 Grey 22975 20% Glass Filled PA66 FR (Dry) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3UG4 LS BK 23215 20% Glass Filled PA66 FR (Conditioned) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3UG4 LS Grey 22985 20% Glass Filled PA66 FR (Conditioned) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Conditioned) Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Dry) Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3WG6 GP BK 23210 30% Glass Filled PA6 (Dry) Description: 30% Glass fiber reinforced and heat aging resistant injection molding grade used e.g. for automobile manifold.Information provided by BASF |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Conditioned) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |
|||
Decomposition Temperature | >= 300 °C | >= 572 °F | |
BASF Ultramid® B3WG5 BK 00564 25% Glass Filled PA6 (Conditioned) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |