Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 50.8 mm/min | 2.00 in/min | FVSS302/SAE J369 in/min |
Kraton® G7705 GI-B (SEBS) Compound Description: Kraton G7705 GI-B is an easy processing, general purpose 44 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Flame Spread | 50.8 mm/min | 2.00 in/min | FVSS302/SAE J369 in/min |
Kraton® G7705 GI-N (SEBS) Compound Description: Kraton G7705 GI-N is an easy processing, general purpose 44 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Flame Spread | 50.8 mm/min | 2.00 in/min | Pass: Burn Rate- Max 100; FMVSS 302 |
Teknor Apex TEKRON® 4300LM-P88-1 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Flame Spread | 50.8 mm/min | 2.00 in/min | FVSS302/SAE J369 in/min |
Kraton® G7720 GI-N (SEBS) Compound Description: Kraton G7720 GI-N is an easy processing, general purpose 57 Shore a hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |