Thermal Properties Metric English Comments
CTE, linear 80.0 - 110 µm/m-°C

@Temperature 20.0 °C
44.4 - 61.1 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Polimersan Plastics POLITEF® (PTFE) with 25% Carbon
As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv..
CTE, linear 80.0 - 110 µm/m-°C

@Temperature 20.0 °C
44.4 - 61.1 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Polimersan Plastics POLITEF® (PTFE) with 25% Carbon
As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv..
CTE, linear 90.0 - 110 µm/m-°C
50.0 - 61.1 µin/in-°F
Polykemi
Polykemi AB POLYfill PP CQX15015 R3 UV Polypropylene, Mineral Reinforced, Scratch Resistant
Information provided by Polykemi AB
CTE, linear 3.00 - 110 µm/m-°C
1.67 - 61.1 µin/in-°F
Average value: 23.2 µm/m-°C Grade Count:47
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu..
CTE, linear 30.0 - 110 µm/m-°C
16.7 - 61.1 µin/in-°F
Average value: 68.9 µm/m-°C Grade Count:12
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar..
CTE, linear 40.0 - 110 µm/m-°C
22.2 - 61.1 µin/in-°F
Average value: 80.3 µm/m-°C Grade Count:13
Overview of materials for Acetal Copolymer, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values ..
CTE, linear 28.8 - 110 µm/m-°C
16.0 - 61.1 µin/in-°F
Average value: 85.4 µm/m-°C Grade Count:32
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is ..
CTE, linear 68.0 - 110 µm/m-°C
37.8 - 61.1 µin/in-°F
Average value: 87.8 µm/m-°C Grade Count:28
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and ..
CTE, linear 50.0 - 110 µm/m-°C
27.8 - 61.1 µin/in-°F
Average value: 68.2 µm/m-°C Grade Count:24
Overview of materials for Polypropylene with 20% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are ..
CTE, linear 14.4 - 110 µm/m-°C
8.00 - 61.1 µin/in-°F
Average value: 35.9 µm/m-°C Grade Count:53
Overview of materials for Nylon 6, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values..
CTE, linear 80.0 - 110 µm/m-°C
44.4 - 61.1 µin/in-°F
ASTM D696
Guarniflon PTFE G456 Polytetrafluoroethylene 25% Hard Carbon
PTFE G Special Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high w..
CTE, linear 75.0 - 110 µm/m-°C
41.7 - 61.1 µin/in-°F
ASTM D696
Guarniflon PTFE G405 Polytetrafluoroethylene 25% Glass Fiber
PTFE G Standard Compound with glass fiberProperties: Enhanced wear resistance. Enhanced chemical resistance (except for alkali and hydrofluoric acid).Applications: Valve seats, seals, bearings, re..
CTE, linear 80.0 - 110 µm/m-°C
44.4 - 61.1 µin/in-°F
ISO 11359
Styrolution Luran® S 767KE ASA
Luran S 767KE is particular suitable for co-extrusion with PVC at low temperature. Hereby, it provides a glossy surface finish.Enhanced flowabilitySuitable for co-extrusion with PVCEnables high glos..
CTE, linear 80.0 - 110 µm/m-°C
44.4 - 61.1 µin/in-°F
ISO 11359
Styrolution Terluran® EGP-7 ABS
Terluran EGP-7 is an extrusion grade with well balanced properties.UL 94 HBInformation provided by Styrolution
CTE, linear 80.0 - 110 µm/m-°C
44.4 - 61.1 µin/in-°F
ISO 11359
Styrolution Terluran® HI-12 ABS
Terluran HI-12 is an injection molding grade of ABS with a very high toughness and easy flow.Very high toughnessEasy flowingUL 94 HB (1.6 & 3.2 mm)Information provided by Styrolution
CTE, linear 80.0 - 110 µm/m-°C
44.4 - 61.1 µin/in-°F
ISO 11359
Styrolution Terluran® GP-25 ABS
Terluran GP-25 is an easy-flow, general purpose injection molding grade with high resistance to impact and heat distortion; intended for a wide range of applications, particularly in the housings se..
CTE, linear 80.0 - 110 µm/m-°C
44.4 - 61.1 µin/in-°F
ISO 11359
Styrolution Terlux® HD 2822 MABS
Terlux® HD 2822 is a new standard-injection molding grade based on a MABS polymer. Terlux® HD 2822 offers a well balanced combination of stiffness and toughness and the high transparency well ..
CTE, linear 81.0 - 110 µm/m-°C

@Temperature 20.0 °C
45.0 - 61.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Westlake Plastics Pomalux® Acetal Copolymer For Medical Applications
Medical grade Pomalux is made from acetal copolymer resin which allows machined products the ability to retain dimensional integrity, maintain stability in water and most chemicals at elevated tempe..
CTE, linear 60.0 - 110 µm/m-°C
33.3 - 61.1 µin/in-°F
Average value: 73.5 µm/m-°C Grade Count:20
Overview of materials for Acrylic, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
CTE, linear 21.6 - 110 µm/m-°C
12.0 - 61.1 µin/in-°F
Average value: 66.6 µm/m-°C Grade Count:27
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..
Copyright © lookpolymers.com All Rights Reserved