Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 210 µm/m-°C @Temperature 20.0 °C |
117 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials RTV627 Dark Gray General Purpose Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
CTE, linear | 210 µm/m-°C @Temperature 20.0 °C |
117 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials RTV6428 Dark Gray General Purpose Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |
|||
CTE, linear | 210 µm/m-°C | 117 µin/in-°F | Above Tg |
Tra-Con Tra-Cast 3156 General Purpose Epoxy Casting System TRA-CAST 3156 is an easy-to-use, low cost, versatile epoxy resin and hardener system developed for general purpose casting applications. It develops excellent adhesion to most metals, plastics, and .. |
|||
CTE, linear | 211 µm/m-°C | 117 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® 301-2FL Low Stress, Optical Epoxy Product Description: EPO-TEK® 301-2FL is a two component optical, medical, and semiconductor grade epoxy resin. It is a more flexible version of EPO-TEK® 301-2.Advantages & Application Notes: Sug.. |
|||
CTE, linear | 210 µm/m-°C | 117 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® 377 High Temperature Epoxy Product Description: EPO TEK®377 is a two component, high Tg, fiber optic grade epoxy adhesive. It is well suited for semiconductor, medical and optical applications.Advantages & Application Notes:.. |
|||
CTE, linear | 210 µm/m-°C | 117 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® OE101 Two Component Epoxy Material Description: A two component epoxy designed for low stress applications in fiber optic packaging, opto-electronics and semiconductors. It is a lower modulus version of EPO-TEK® 353ND.Inf.. |
|||
CTE, linear | 210 µm/m-°C @Temperature -40.0 - 140 °C |
117 µin/in-°F @Temperature -40.0 - 284 °F |
ASTM D696 |
Arkema Group Pebax® 3533 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
CTE, linear | 210 µm/m-°C @Temperature 20.0 °C |
117 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials RTV630 Blue General Purpose Potting/Encapsulating Compound Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth.. |