CTE, linear 14.4 µm/m-°C

@Temperature -20.0 - 150 °C
8.00 µin/in-°F

@Temperature -4.00 - 302 °F
ASTM E831
Polymer Resources PEI-G40 Polyetherimide, 40% Glass Reinforced
Polyetherimide, 40% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly..
CTE, linear 14.4 µm/m-°C

@Temperature 20.0 °C
8.00 µin/in-°F

@Temperature 68.0 °F
ASTM D696
PolyOne Edgetek® PK-30CF/000 Polyetheretherketone (PEEK), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
CTE, linear 14.4 - 21.6 µm/m-°C
8.00 - 12.0 µin/in-°F
Average value: 18.9 µm/m-°C Grade Count:4
Overview of materials for Polyetherimide (PEI), 40% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 40% Glass Fiber". Specific grades with glass content between 35% and 44% are included. E..
CTE, linear 14.4 - 110 µm/m-°C
8.00 - 61.1 µin/in-°F
Average value: 35.9 µm/m-°C Grade Count:53
Overview of materials for Nylon 6, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values..
CTE, linear 14.4 - 16.2 µm/m-°C
8.00 - 9.00 µin/in-°F
Average value: 15.5 µm/m-°C Grade Count:3
Overview of materials for Nylon 610, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of..
CTE, linear 14.4 µm/m-°C
8.00 µin/in-°F
IBC Advanced Alloys 41C Beryllium Nickel Casting Alloy
Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th..
CTE, linear 14.4 µm/m-°C
8.00 µin/in-°F
IBC Advanced Alloys 42C Beryllium Nickel Casting Alloy
Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th..
CTE, linear 14.4 µm/m-°C
8.00 µin/in-°F
IBC Advanced Alloys 43C Beryllium Nickel Casting Alloy
Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th..
CTE, linear 14.4 µm/m-°C
8.00 µin/in-°F
IBC Advanced Alloys 44C Beryllium Nickel Casting Alloy
Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th..
CTE, linear 14.4 µm/m-°C
8.00 µin/in-°F
IBC Advanced Alloys 46C Beryllium Nickel Casting Alloy
Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th..
CTE, linear 14.4 µm/m-°C
8.00 µin/in-°F
IBC Advanced Alloys FA230 Beryllium Nickel Casting Alloy
Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th..
CTE, linear 14.4 µm/m-°C

@Temperature 20.0 °C
8.00 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Techmer ES Electrafil® J-1/CF/30 Nylon 66, 30% Carbon Fiber Reinforced
Carbon Fiber Reinforced
CTE, linear 14.4 µm/m-°C

@Temperature 20.0 °C
8.00 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Techmer ES Electrafil® J-1/CF/30/TF/15 Nylon 66, 30% Carbon Fiber Reinforced, PTFE Lubed
Carbon Fiber Reinforced, PTFE Lubricated
CTE, linear 14.4 µm/m-°C

@Temperature 20.0 °C
8.00 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Techmer ES Electrafil® J-1/CF/40 BK PA66
CTE, linear 14.4 µm/m-°C

@Temperature 20.0 °C
8.00 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Techmer ES Electrafil® J-1/CF/40 NAT PA66
CTE, linear 14.4 µm/m-°C

@Temperature 20.0 - 100 °C
8.00 µin/in-°F

@Temperature 68.0 - 212 °F
Special Metals INCOLOY® Alloy 800
A nickel-iron-chromium alloy with good strength and excellent resistance to oxidation and carburization in high-temperature atmospheres. It also resists corrosion by many aqueous environments. The..
CTE, linear 14.4 µm/m-°C

@Temperature 20.0 - 100 °C
8.00 µin/in-°F

@Temperature 68.0 - 212 °F
Special Metals INCOLOY® Alloy 800HT™
A nickel-iron-chromium alloy having the same basic composition as INCOLOY alloy 800 but with significantly higher creep-rupture strength. The higher strength results from close control of the carbo..
CTE, linear 14.4 µm/m-°C
8.00 µin/in-°F
ASTM-D696
CoorsTek PolyGlyde™ 5400 Self-Lubricating Seal
PolyGlyde seals offer low heat generation in high-friction and high-stress environments. These seals provide superior performance over traditional carbon materials: runs cooler – even in dry-runni..
CTE, linear 14.4 µm/m-°C

@Temperature 20.0 °C
8.00 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Ensinger Tecapeek® CF30 Polyetheretherketone, 30% Carbon Reinforced (PEEK)
Tecapeek™, made from Victrex® PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance. Excellent ..
CTE, linear 14.4 µm/m-°C
8.00 µin/in-°F
ASTM D696
Ensinger Tecapeek® MT CF 30 Polyetheretherketone (PEEK)
TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti..
CTE, linear 14.4 - 16.2 µm/m-°C
8.00 - 9.00 µin/in-°F
Average value: 14.8 µm/m-°C Grade Count:4
Overview of materials for Nylon 66, 40% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Carbon Fiber Filled". Specific grades with carbon fiber content between 35% and 44% are in..
CTE, linear 14.4 µm/m-°C

@Temperature 20.0 °C
8.00 µin/in-°F

@Temperature 68.0 °F
ASTM D696
PolyOne Edgetek® NI-40CF/000 Nylon 6/10 - 40% Carbon Fiber Reinforced  (discontinued **)
Data provided by PolyOne.
CTE, linear 14.4 µm/m-°C

@Temperature 20.0 °C
8.00 µin/in-°F

@Temperature 68.0 °F
ASTM D696
PolyOne Edgetek® PI-40GF/000 Polyetherimide (PEI), Glass Filled  (discontinued **)