Polymer Property : CTE, linear = 147 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 147 µm/m-°C

@Temperature 20.0 °C
81.7 µin/in-°F

@Temperature 68.0 °F
Teknor Apex TEKRON® 4300LM-P88-1 Thermoplastic Elastomer
Information provided by Teknor Apex Company
CTE, linear 147 µm/m-°C

@Temperature 20.0 °C
81.7 µin/in-°F

@Temperature 68.0 °F
Teknor Apex TEKRON® 4300LM-P96-1 Thermoplastic Elastomer
Information provided by Teknor Apex Company
CTE, linear 147 µm/m-°C
81.7 µin/in-°F
Above Tg
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
CTE, linear 147 µm/m-°C
81.7 µin/in-°F
90 Minute UV Cure; T>Tg; ASTM E831-93
3D Systems Accura® SI 40 Plastic for the SLA® 250 System
Accura 40 "Ar" or "Hc" type materials - for the SLA 250 system. Mimics Nylon 6:6ApplicationsHigh temperature testing:Under hood bolt-on testingWind tunnel testingHVAC testingPrototyping and testing ..