Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 4.00 - 275 µm/m-°C | 2.22 - 153 µin/in-°F | Average value: 62.6 µm/m-°C Grade Count:110 |
Overview of materials for Epoxy Encapsulant, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o.. |