Polymer Property : CTE, linear = 20.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 36.0 µm/m-°C

@Temperature 20.0 °C
20.0 µin/in-°F

@Temperature 68.0 °F
North Wood Plastics Polypropylene with 60% Wood Fiber, Extrusion Grade
Data provided by North Wood Plastics, Inc.
CTE, linear 36.0 µm/m-°C

@Temperature 20.0 °C
20.0 µin/in-°F

@Temperature 68.0 °F
North Wood Plastics Polypropylene with 60% Wood Fiber, Molding Grade
Data provided by North Wood Plastics, Inc.
CTE, linear 36.0 µm/m-°C

@Temperature 20.0 °C
20.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Ravago Manufacturing Americas Hylon® N2017THL Nylon 6 (DAM)
Information provided by Ravago.
CTE, linear 36.0 µm/m-°C

@Temperature -40.0 - 149 °C
20.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP Duratron® PAI T4501 Polyamide-imide, compression molded bearing grade (ASTM Product Data Sheet)
CTE, linear 36.0 µm/m-°C

@Temperature -40.0 - 149 °C
20.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP Duratron® PAI T4540 Polyamide-imide, compression molded (ASTM Product Data Sheet)
CTE, linear 36.0 µm/m-°C

@Temperature 20.0 °C
20.0 µin/in-°F

@Temperature 68.0 °F
North Wood Plastics HDPE with 60% Wood Fiber
Data provided by North Wood Plastics, Inc.
CTE, linear 36.0 µm/m-°C

@Temperature 20.0 °C
20.0 µin/in-°F

@Temperature 68.0 °F
North Wood Plastics PS with 40% Wood Fiber
Data provided by North Wood Plastics, Inc.
CTE, linear 36.0 - 99.0 µm/m-°C
20.0 - 55.0 µin/in-°F
Average value: 64.3 µm/m-°C Grade Count:3
Overview of materials for High Density Polyethylene (HDPE), Wood Filled
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Wood Filled". Each property range of values reported is minimum and ma..
CTE, linear 36.0 - 216 µm/m-°C
20.0 - 120 µin/in-°F
Average value: 139 µm/m-°C Grade Count:76
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..
CTE, linear 36.0 µm/m-°C

@Temperature 20.0 °C
20.0 µin/in-°F

@Temperature 68.0 °F
Z-direction; ASTM D696
Premix Premi-Glas® 1265 VE 1265-VE (Injection Compression Molded) Glass Reinforced Vinyl Ester TMC  (discontin
Description: Premi-Glas® 1265 VE is a glass reinforced vinyl ester molding compound designed for automotive under the hood applications. Key features and benefits: Designed for Injection or Injecti..
CTE, linear 36.0 µm/m-°C

@Temperature 20.0 °C
20.0 µin/in-°F

@Temperature 68.0 °F
Z-direction; ASTM D696
Premix Premi-Glas® 2200-22 Fiberglass Reinforced SMC  (discontinued **)
Description: Premi-Glas® 2200-22 is a fiberglass reinforced thermoset Sheet Molding Compound similar to the Premi-Glas® 2200-22 CR-SX product. Unlike the -CR-SX version, this product carries no UL..
CTE, linear 36.0 µm/m-°C

@Temperature 20.0 °C
20.0 µin/in-°F

@Temperature 68.0 °F
Z-direction; ASTM D696
Premix Premi-Glas® 8102-13 Glass Reinforced Polyester BMC  (discontinued **)
Description: Premi-Glas® 8102-13 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits:..
CTE, linear 36.0 µm/m-°C

@Temperature 20.0 °C
20.0 µin/in-°F

@Temperature 68.0 °F
Z-direction; ASTM D696
Premix Premi-Glas® 8102-20 Glass Reinforced Polyester BMC  (discontinued **)
Description: Premi-Glas® 8102-20 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits:..
CTE, linear 36.0 µm/m-°C

@Temperature 20.0 °C
20.0 µin/in-°F

@Temperature 68.0 °F
Z-direction; ASTM D696
Premix Premi-Glas® 8105 Glass Reinforced Polyester BMC  (discontinued **)
Description: Premi-Glas® 8105 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits: Ex..
CTE, linear 36.0 µm/m-°C

@Temperature 20.0 °C
20.0 µin/in-°F

@Temperature 68.0 °F
Indium Corp. Indalloy® 209 Sn-Ag-Sb Solder Alloy
Low temperature die attach alloy. Has very high tensile strength. Old Motorola die attach solder; very brittle.Information provided by the manufacturer, Indium Corporation.
CTE, linear 36.0 µm/m-°C

@Temperature -30.0 - 100 °C
20.0 µin/in-°F

@Temperature -22.0 - 212 °F
ASTM D696
LyondellBasell Hifaxâ„¢ CB272 Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ CB272 high melt flow, 900 MPa flexural modulus, low CLTE, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of rigidity and dime..
CTE, linear 36.0 µm/m-°C

@Temperature 40.0 - 130 °C
20.0 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Plenco 4349 Phenolic, Granular, Injection Molded
PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer ..
CTE, linear 36.0 µm/m-°C
20.0 µin/in-°F
CMT Materials HYTAC® FLXT High Temperature, PTFE Impregnated Copolymer Syntactic
HYTAC-FLXT is a unique material, combining the toughness and higher friction of FLX with improved release characteristic through PTFE impregnation. The result is a new, tough syntactic with just th..
CTE, linear 36.0 µm/m-°C

@Temperature -40.0 - 120 °C
20.0 µin/in-°F

@Temperature -40.0 - 248 °F
ASTM E831
Azdel AZMET® CM32350 35% continuous random fiber mat / PET resin matrix
AZDEL® CM20350 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a Polyethylene Terephthalate (PET) resin matrix. This composite material fea..
CTE, linear 36.0 µm/m-°C

@Temperature -40.0 - 120 °C
20.0 µin/in-°F

@Temperature -40.0 - 248 °F
ASTM E831
Azdel Plus C321-B01 32% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C321-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow prope..
CTE, linear 36.0 µm/m-°C

@Temperature 20.0 °C
20.0 µin/in-°F

@Temperature 68.0 °F
Armstrong C-1/H20 Epoxy Adhesive
A versatile, low viscosity, unfilled resin used for electrical potting and laminating applications. It is an excellent insulator, and provides outstanding chemical resistance to most compoundsInfor..
CTE, linear 36.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
20.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
Beijing Chemical Industry KAIFA® 304-G20 PBT Resin
20% glass fiber reinforced, flame retardant, low bleeding, UV-resistantInformation provided by Beijing Chemical Industry Research Institute (Group)
CTE, linear 36.0 - 45.0 µm/m-°C
20.0 - 25.0 µin/in-°F
ASTM D696
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug..
CTE, linear 36.0 - 50.0 µm/m-°C
20.0 - 27.8 µin/in-°F
Average value: 43.2 µm/m-°C Grade Count:5
Overview of materials for Polyphenylene Ether, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu..
CTE, linear 36.0 µm/m-°C

@Temperature 23.0 - 100 °C
20.0 µin/in-°F

@Temperature 73.4 - 212 °F
Quadrant EPP Duratron® PI D7015G PI, bearing grade (ISO Data)
This grade contains 15 % graphite, added to provide long wear and low friction Good performance at elevated temperature (>425 °C) Good chemical resistance Easily machined from a broad range of shap..
CTE, linear 36.0 µm/m-°C

@Temperature 20.0 °C
20.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
PolyOne Edgetek® PS-20GF/000 FR Polybutylene Terephthalate (PBT), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedIgnition ResistantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.