Polymer Property : CTE, linear = 22.2 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 20.0 - 40.0 µm/m-°C

@Temperature 50.0 - 150 °C
11.1 - 22.2 µin/in-°F

@Temperature 122 - 302 °F
ISO 11359-2
Raschig Group 4552 Silicone
Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to +/- 300°C continuously, excellent electrical properties, good mechanical strength, very good dimensional stabi..
CTE, linear 15.0 - 40.0 µm/m-°C
8.33 - 22.2 µin/in-°F
Average value: 21.9 µm/m-°C Grade Count:9
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35..
CTE, linear 20.0 - 40.0 µm/m-°C
11.1 - 22.2 µin/in-°F
Average value: 30.5 µm/m-°C Grade Count:15
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a..
CTE, linear 18.0 - 40.0 µm/m-°C
10.0 - 22.2 µin/in-°F
Average value: 28.8 µm/m-°C Grade Count:9
Overview of materials for Polycarbonate, Carbon + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum valu..
CTE, linear 20.0 - 40.0 µm/m-°C

@Temperature 50.0 - 150 °C
11.1 - 22.2 µin/in-°F

@Temperature 122 - 302 °F
Average value: 30.0 µm/m-°C Grade Count:2
Overview of materials for Silicone, Molded, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..
CTE, linear 15.0 - 40.0 µm/m-°C
8.33 - 22.2 µin/in-°F
Average value: 29.4 µm/m-°C Grade Count:11
Overview of materials for Phenolic, Novolac, Fabric Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Fabric Filled". Each property range of values reported is minimum and maximum values ..
CTE, linear 30.0 - 40.0 µm/m-°C

@Temperature 20.0 - 100 °C
16.7 - 22.2 µin/in-°F

@Temperature 68.0 - 212 °F
DIN 53752
Schwartz Technical Plastics LAMINEX® 2101 Cotton Fabric, Phenolic Resin Impregnated
Application: bearing segments and prismatic bearingsInformation provided by Schwartz Technical Plastics GmbH
CTE, linear 30.0 - 40.0 µm/m-°C

@Temperature 20.0 - 100 °C
16.7 - 22.2 µin/in-°F

@Temperature 68.0 - 212 °F
DIN 53752
Schwartz Technical Plastics LAMINEX® 2141 Cotton Fabric, Phenolic Resin Impregnated, MoS2 Filled
Application: bearing segments and prismatic bearingsInformation provided by Schwartz Technical Plastics GmbH
CTE, linear 35.0 - 40.0 µm/m-°C
19.4 - 22.2 µin/in-°F
Master Bond EP42HT-2Med Epoxy Meets USP Class VI Requirements
Description: Master Bond Polymer System EP42HT-2Med is a room temperature curable two component epoxy, adhesive, sealant, coating and casting material featuring high temperature resistance along wit..
CTE, linear 35.0 - 40.0 µm/m-°C
19.4 - 22.2 µin/in-°F
Master Bond EP42HT-2ND-2Med Heat Resistant, Medical Grade Non-Drip Epoxy
Master Bond Polymer System EP42HT-2ND2MED (Black) is a room temperature curable two component epoxy adhesive and sealant featuring high temperature resistance along with outstanding chemical resista..
CTE, linear 35.0 - 40.0 µm/m-°C
19.4 - 22.2 µin/in-°F
Master Bond EP45HTND-2 Chemically Resistant, Non-Drip Epoxy
Description: Master Bond EP45HTND-2 is a two component epoxy system for high performance bonding, sealing and coating. It is used for applications requiring solid temperature resistance and capable ..
CTE, linear 35.0 - 40.0 µm/m-°C
19.4 - 22.2 µin/in-°F
Master Bond EP42-2LV Epoxy Resists Heat and Chemicals
Description: Master Bond Polymer System EP42-2LV is a low viscosity room temperature curable two component epoxy, adhesive, sealant, coating and casting material featuring outstanding chemical resis..
CTE, linear 35.0 - 40.0 µm/m-°C
19.4 - 22.2 µin/in-°F
Master Bond EP42HT-2 Epoxy Adhesive Resists Sterilization
Description: Master Bond Polymer System EP42HT-2 is a room temperature curable, two component epoxy adhesive, sealant, coating and casting material featuring high temperature resistance along with o..
CTE, linear 35.0 - 40.0 µm/m-°C
19.4 - 22.2 µin/in-°F
Master Bond EP42HT-2FG Two Component Epoxy Adhesive for Food Applications
Master Bond Polymer System EP42HT-2FG is a room temperature setting, two component epoxy adhesive, sealant and coating specially formulated for food applications. It has been independently tested an..
CTE, linear 35.0 - 40.0 µm/m-°C
19.4 - 22.2 µin/in-°F
Master Bond Supreme 11AOHTLO Epoxy Passes NASA Low Outgassing Tests
Description: Master Bond Supreme 11AOHTLO is a two component epoxy resin system for high performance bonding and sealing. Although, it is formulated to cure at room temperature, the best cure schedu..
CTE, linear 35.0 - 40.0 µm/m-°C
19.4 - 22.2 µin/in-°F
ASTM D696
Unitika PT-3020
Characteristics: Dimensional accuracy (planarity) Heat resistance Creep resistance and elasticity RigidityInformation provided by Unitika Ltd.
CTE, linear 30.0 - 40.0 µm/m-°C

@Temperature 20.0 °C
16.7 - 22.2 µin/in-°F

@Temperature 68.0 °F
ASTM D696
E-Polymers TEKAMID® TA210M40 , 40% Mineral Filled PA66, DAM
40% Mineral filled, Heat resistance, PlatableInformation provided by E-Polymers Co. Ltd.
CTE, linear 20.0 - 40.0 µm/m-°C
11.1 - 22.2 µin/in-°F
Average value: 27.7 µm/m-°C Grade Count:14
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an..
CTE, linear 30.0 - 40.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
16.7 - 22.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics NORYL PX2944 PPE+HIPS (Asia Pacific)
PPE/PS, GF20%, high heat, non-FR
CTE, linear 35.0 - 40.0 µm/m-°C
19.4 - 22.2 µin/in-°F
Master Bond EP42HT-2LO Low Outgassing, Heat Resistant Two Component Epoxy
Master Bond Polymer System EP42HT-2LO is a room temperature curable two component epoxy, adhesive, sealant, coating and casting material featuring high temperature resistance along with outstanding ..
CTE, linear 32.0 - 40.0 µm/m-°C

@Temperature 100 - 300 °C
17.8 - 22.2 µin/in-°F

@Temperature 212 - 572 °F
Average value: 37.4 µm/m-°C Grade Count:27
Overview of materials for Polyimide, Thermoset Film
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appr..