Polymer Property : CTE, linear = 25.6 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 46.0 µm/m-°C

@Temperature -30.0 - 100 °C
25.6 µin/in-°F

@Temperature -22.0 - 212 °F
ASTM D696
LyondellBasell Hifaxâ„¢ CB285 Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ CB285 high melt flow, 1,300 MPa flexural modulus, low CLTE, UV-stabilized, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of ..
CTE, linear 46.0 µm/m-°C

@Temperature 40.0 - 130 °C
25.6 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Plenco 1501 Polyester, Pellet, Injection Molded
PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va..
CTE, linear 46.0 µm/m-°C
25.6 µin/in-°F
ASTM D696
Unitika AXG-1500-300 Dry
Characteristics: Glass-reinforced grades of the AX1500 resin, excellent in heat and chemical resistancesFavorable rigidity and dimensional accuracyInformation provided by Unitika Ltd.
CTE, linear 46.0 µm/m-°C

@Temperature 40.0 - 130 °C
25.6 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Plenco 4466 Phenolic, Granular, Injection Molded
PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466..
CTE, linear 46.0 µm/m-°C

@Temperature 20.0 °C
25.6 µin/in-°F

@Temperature 68.0 °F
Cosmic Plastics K43 Mineral Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
CTE, linear 46.0 µm/m-°C

@Temperature 40.0 - 130 °C
25.6 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Plenco 5488 Phenolic, Granular, Injection Molded
PLENCO 05488 is a woodflour and graphite filled phenolic molding compound offering improved abrasion resistance. UL recognized under component file E40654. 05488 is available in brown. 05488 is not ..
CTE, linear 46.0 µm/m-°C

@Temperature 40.0 - 130 °C
25.6 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Plenco 4300 Phenolic, Granular, Injection Molded
PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric..
CTE, linear 46.0 µm/m-°C

@Temperature 40.0 - 130 °C
25.6 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Plenco 4300 Phenolic, Granular, Transfer Molded
PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric..
CTE, linear 46.0 µm/m-°C
25.6 µin/in-°F
Below Tg
Epoxy Technology EPO-TEK® TV1002 Polyimide Adhesive
Material Description: A single component, screen printable polyimide adhesive designed for semiconductor wafer passivation applications. It is a high temperature chemistry capable of resisting >400..
CTE, linear 46.0 µm/m-°C
25.6 µin/in-°F
x direction
Arlon IsoClad 917 Non-Woven Fiberglass Reinforced PTFE
Traditional - Highest Performance, PTFE Coated Light Woven Glass Styles, Interdispersed PTFE FilmInformation provided by Arlon Materials for Electronics (MED).
CTE, linear 46.0 µm/m-°C

@Temperature 20.0 °C
25.6 µin/in-°F

@Temperature 68.0 °F
Armstrong A-31 Epoxy Adhesive
Is a neutral-colored thixotropic paste material having a creamy or buttery consistency that will not flow even when cured at elevated temperatures A-31 also features Extremely low outgassing charact..
CTE, linear 46.0 µm/m-°C

@Temperature 20.0 °C
25.6 µin/in-°F

@Temperature 68.0 °F
Armstrong A-40 Epoxy Adhesive
Is a high viscosity, dark gray, liquid adhesive system that is qualified under Mil. Spec. MMM-A-134, Type II. NOTE: Adhesives qualified under this Specification (A-40, A-706) feature exceptional re..
CTE, linear 46.0 µm/m-°C
25.6 µin/in-°F
below Tg
Gromax Evasin EV-3201V Ethylene-Vinyl Alcohol Copolymer
Unmodified random Co-Polymer of [Ethylene-Vinyl alcohol], designed for therm-plastic processing into Sheets and Foils with high Oxygen and Aroma Barrier EffectInformation provided by Gromax Enterpri..
CTE, linear 46.0 µm/m-°C

@Temperature 40.0 - 130 °C
25.6 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Plenco 7579 Phenolic, Granular, Injection Molded
PLENCO 07579 is a fast curing, woodflour filled, novolac phenolic molding compound, formulated for industrial applications that do not require a smooth finish. UL recognized under component file E40..
CTE, linear 46.0 - 52.0 µm/m-°C

@Temperature 40.0 - 130 °C
25.6 - 28.9 µin/in-°F

@Temperature 104 - 266 °F
Average value: 48.0 µm/m-°C Grade Count:3
Overview of materials for Phenolic, Novolac, Mineral/Cellulose Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Cellulose Filled". Each property range of values reported is minimum and maxi..