Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 22.0 - 500 µm/m-°C | 12.2 - 278 µin/in-°F | Average value: 83.0 µm/m-°C Grade Count:13 |
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are.. |
|||
CTE, linear | 11.0 - 500 µm/m-°C @Temperature 55.0 - 250 °C |
6.11 - 278 µin/in-°F @Temperature 131 - 482 °F |
Average value: 122 µm/m-°C Grade Count:8 |
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are.. |
|||
CTE, linear | 12.0 - 500 µm/m-°C | 6.67 - 278 µin/in-°F | Average value: 104 µm/m-°C Grade Count:15 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |
|||
CTE, linear | 8.00 - 500 µm/m-°C @Temperature 55.0 - 250 °C |
4.44 - 278 µin/in-°F @Temperature 131 - 482 °F |
Average value: 161 µm/m-°C Grade Count:9 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |
|||
CTE, linear | 10.8 - 500 µm/m-°C | 6.00 - 278 µin/in-°F | Average value: 97.0 µm/m-°C Grade Count:9 |
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim.. |
|||
CTE, linear | 90.0 - 500 µm/m-°C @Temperature -20.0 - 100 °C |
50.0 - 278 µin/in-°F @Temperature -4.00 - 212 °F |
Average value: 295 µm/m-°C Grade Count:1 |
Overview of materials for Medium Density Polyethylene (MDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Molded". Each property range of values reported is minimum and maxim.. |
|||
CTE, linear | 10.0 - 500 µm/m-°C | 5.56 - 278 µin/in-°F | Average value: 55.8 µm/m-°C Grade Count:37 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
CTE, linear | 10.0 - 500 µm/m-°C | 5.56 - 278 µin/in-°F | Average value: 70.1 µm/m-°C Grade Count:46 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |
|||
CTE, linear | 14.0 - 500 µm/m-°C @Temperature 55.0 - 160 °C |
7.78 - 278 µin/in-°F @Temperature 131 - 320 °F |
Average value: 154 µm/m-°C Grade Count:6 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |
|||
CTE, linear | 90.0 - 500 µm/m-°C @Temperature -20.0 - 100 °C |
50.0 - 278 µin/in-°F @Temperature -4.00 - 212 °F |
Average value: 295 µm/m-°C Grade Count:1 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |
|||
CTE, linear | 10.0 - 500 µm/m-°C | 5.56 - 278 µin/in-°F | Average value: 153 µm/m-°C Grade Count:22 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |
|||
CTE, linear | 4.00 - 500 µm/m-°C @Temperature 55.0 - 160 °C |
2.22 - 278 µin/in-°F @Temperature 131 - 320 °F |
Average value: 376 µm/m-°C Grade Count:3 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |
|||
CTE, linear | 16.0 - 500 µm/m-°C | 8.89 - 278 µin/in-°F | Average value: 183 µm/m-°C Grade Count:12 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
CTE, linear | 500 - 500 µm/m-°C @Temperature 55.0 - 160 °C |
278 - 278 µin/in-°F @Temperature 131 - 320 °F |
Average value: 500 µm/m-°C Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |